Ti-6Al-7Nb Titanium Alloy Bar (ASTM F1295 / ISO 5832-11)

Ti-6Al-7Nb Titanium Alloy Bar (ASTM F1295 / ISO 5832-11)

Ti-6Al-7Nb Titanium Alloy Bar is a dedicated high-strength titanium alloy with excellent biocompatibility for surgical implants. double or triple vacuum melted to provide an ingot composition that is very uniform and homogeneous.
Send Inquiry

Lork Group is a reliable manufacturer and supplier of Ti-6Al-7Nb Titanium Alloy Bar (ASTM F1295 / ISO 5832-11) in China. Titanium Ti6Al-7Nb was developed for use in medical and surgical device applications, although its properties are nearly identical to Ti6Al4V; however, Niobium has been substituted for Vanadium as the beta-stabilising agent, giving improved biocompatibility.

 

Ti-6Al-7Nb titanium alloy is an 'upgraded solution' specifically designed for high-end medical device projects with stringent requirements for the long-term biocompatibility of implants or concerns regarding specific elements (such as vanadium).

 

Ti-6Al-7Nb (commonly known as 'Grade 7 titanium') is based on Ti-6Al-4V, but with a crucial strategic substitution: niobium (Nb), which offers greater bioinertness, completely replaces the potentially controversial vanadium (V). This makes it the "ceiling" of biocompatibility in the titanium alloy family for medical applications, meaning it is the best material for long-term or permanent implantable hip, knee, and spinal fixation systems. Furthermore, its exceptional corrosion resistance in fluorine-containing environments, a quality that can be described as a "lock," is also a key reason why it is more suitable for dental implants than Ti-6Al-4V.

 

Price Concerns Answered

 

One question our past clients have often asked is, "How much more expensive is it than Ti-6Al-4V?"

 

  • The answer is a definite yes:

"Yes, because niobium metal is significantly more expensive than vanadium, and the smelting control requirements are much higher, the raw material cost of Ti-6Al-7Nb is approximately 1.5 to 2 times that of Ti-6Al-4V."

 

  • However, behind the price lies value:

 

Product Differentiation Value: When your competitors are all using Ti-6Al-4V, using Ti-6Al-7Nb allows your product to establish a unique marketing and technological barrier based on "superior biocompatibility," supporting a higher brand positioning and selling price.

 

Risk Mitigation Value: It completely avoids any academic controversies or future regulatory risks regarding "potential risks of vanadium ions," providing your product with "future-proven" safety.

 

Registration Support Value: For products targeting high-end markets such as the EU and the US, using this more academically recognized biocompatible material may be more persuasive and facilitate a smoother process during clinical evaluations and registration applications.

"Therefore, choosing Ti-6Al-7Nb is not just choosing a material, but choosing a future-oriented, life-responsible product strategy. It is particularly suitable for applications in high-end spine, joint, dental implant, and pacemaker housings-fields with stringent long-term safety requirements. We are not only your supplier, but also your 'materials strategic partner' in this professional field."

 

Finally, based on our comprehensive inventory and customer base, we will consider providing you with information (application case studies from a well-known orthopedic company we have collaborated with - after desensitization) and remaining material samples. You can arrange testing and evaluation first.

 

Chemical Composition

 

Weight %

Al

Nb

Ta

Fe

O

C

N

H

Ti

Titanium 6Al-7nb

5.5-6.6

6.5-7.5

0.50 max

0.25 max

0.20 max

0.08 max

0.05 max

0.009 max

Bal

 

Our bars strictly adhere to ASTM F1295 / ISO 5832-11 standards.

 

Mechanical properties

 

Typical performance in the annealed state

 

Typical performance annealed state
Tensile strength: ≥ 900 MPa (equivalent to Ti-6Al-4V)
Yield strength: ≥ 800 MPa
Elongation: ≥ 10%

 

More importantly, we have excellent control over fatigue strength and fracture toughness data, which fully meets the stringent requirements of cyclic loads on the human skeleton.

 

Procurement Recommendations

 

We aspire to be your "solution partner." Based on our experience from multiple procurement projects of Ti-6Al-7Nb titanium alloy rods over the past three years, we hope this information will be helpful.

 

1. Procurement Specification Recommendations:

"We recommend that you clearly specify on your drawings and technical agreements: 'Ti-6Al-7Nb, UNS R56700, conforming to ASTM F1295 standard, delivered in annealed condition.' We support custom sizes from Φ10mm to Φ150mm and offer precision machining services for bright rods."

Furthermore, we are also planning to manufacture custom sizes. Please contact us with your specific requirements.

 

2. Key Points for Machining:

"In terms of machining, it's similar to Ti-6Al-4V, but one point to note is that its thermal conductivity is slightly lower, and the tendency to stick to the tool is more pronounced. We recommend customers use sharp carbide tools, reduce cutting speed but increase feed rate, and ensure sufficient cooling. We have excellent machining plants we cooperate with that we can recommend."

 

3. Quality Inspection (Our Firewall, Your Peace of Mind):

"We provide a complete Original Material Report (MTR) for each batch of materials, traceable back to the vacuum melting furnace. In addition, after the goods are manufactured, we will arrange quality inspections according to contract requirements, checking for compliance with standards in appearance, surface finish, chemical composition, mechanical properties, dimensional tolerances, etc. Samples, photos, and videos are retained and archived. Besides routine mechanical property testing, we strongly recommend and can assist you in conducting two key tests on each batch of incoming materials:

  • Portable Spectrometer (PMI) Quick Screening: Key Confirmation" Containing niobium (Nb) and being vanadium-free (V) is the bottom line for preventing material mismatch.
  • Third-party biocompatibility testing: Although the material itself meets standards, for first-time collaborations or critical projects, submitting samples to institutions such as SGS or CTI for cytotoxicity testing is a "golden endorsement" for smoother product registration.

 