AMS 5843 MP159 Bar(UNS R30159)

AMS 5843 MP159 Bar(UNS R30159)

MP159 cobalt-nickel alloy bars conforming to AMS 5843 standards (UNS R30159) are high-strength cobalt-nickel-based alloys suitable for demanding aerospace applications. Our MP159 bars are dimensionally precise and centerlessly ground, designed specifically for manufacturing high-strength fasteners, bolts, studs, and other critical components.
Send Inquiry

Products Description

 

MP159 is a high-strength cobalt-nickel-based multiphase alloy, primarily composed of cobalt, nickel, chromium, iron, and molybdenum, with added elements such as titanium, niobium, and aluminum. This alloy achieves extremely high tensile strength, good toughness, and corrosion resistance through solution treatment, cold working, and subsequent aging.

 

AMS 5843 is specifically designed for MP159 alloy bars that have undergone solution treatment, cold working, and aging. Compared to AMS 5841 and AMS 5842, AMS 5843 has higher strength requirements and is suitable for manufacturing aerospace fasteners subjected to high preloads, high mechanical loads, and complex service environments.

 

Bar dimensions and delivery condition

 

Size: AMS 5843 covers high-strength, corrosion-resistant, and heat-resistant cobalt-nickel-chromium alloy bars in nominal diameters of 1-3/4 inches (44.4 mm) and below

Our price is $220-$240 USD, with a minimum order quantity of 100 kg.

Delivery Condition: Solution Heat-Treated + Cold Drawn + Aged

AMS 5843 MP159 Bar

Note: Prices are subject to market fluctuations and processing techniques, and are not fixed. Please contact us for more details.

chemical composition

 

Element Min Max
Nickel remainder  
Boron -- 0.03
Iron 8.00 10.00
Aluminum 0.10 0.30
Titanium 2.50 3.25
Columbium(Niobium) 0.25 0.75
Molybdenum 6.00 8.00
Cobalt 34.00 38.00
Chromium 18.00 20.00

Sulfur

-- 0.010
Phosphorus -- 0.020
Silicon -- 0.20
Manganese -- 0.20
Carbon -- 0.04

 

Minimum room-temperature tensile properties

 

Tensile Strength
1793Mpa
Yield Strength at 0.2% Offset
1724Mpa
Elongation in 4D
6%
Reduction of Area
22%

 

Minimum elevated temperature tensile properties

At 1100 °F (593 °C)
Tensile Strength
1413Mpa
Yield Strength at 0.2% Offset
1310Mpa
Elongation in 4D
5%
Reduction of Area
15%

 

Comparison of MP159 AMS 5841, AMS 5842 and AMS 5843

 

Comparison Projects AMS 5841 AMS 5842 AMS 5843 476PCS
Material MP159 MP159 MP159 420PCS
Product Form Bar Bar Bar 336PCS
Solution heat treatment √ √ √ 302PCS
Cold working strengthening -- √ √ 252PCS
Aging treatment -- -- √  
Final state Solution treatment Solution treatment + cold working Solution treatment + cold working + aging  
Main characteristics High plasticity High strength Ultra-high strength  

If you need to compare the bar stock of the three standards, you can click the image on the right or the blue link to learn more about the bar stock information for the AMS 5841 and AMS 5842 standards.

 

 

AMS 5841 covers solution heat-treated MP159 bars, providing a relatively soft and ductile condition for subsequent processing. AMS 5842 introduces additional cold working to increase strength and hardness. AMS 5843 takes the material one step further by combining solution heat treatment, cold working, and aging to achieve an ultra-high-strength condition.

AMS 5841 MP159 Cobalt Alloy

 

 

Among these three specifications, AMS 5843 is particularly suitable for applications requiring exceptional tensile strength and load-bearing capability, including aerospace fasteners, high-strength bolts, and precision structural components.

AMS 5842 MP159 Cobalt Alloy

 

 Lork Group
 Marketing Operations Department

Hot Tags: MP159 Bar, AMS 5843, UNS R30159, Cobalt-Nickel Alloy, Aerospace Fastener Alloy, High-Strength Cobalt-Nickel Alloy Bar, MP159 Round Bar

Send Inquiry