18Ni250, 18Ni300, and 18Ni350 are grades of 18Ni maraging steel, a long-standing supplier of the Lork Group. 18Ni maraging steel belongs to a family of ultra-high-strength low-carbon steels known for their high nickel content.

 

The designations 250, 300, and 350 refer to their typical minimum yield strength (ksi, kilopounds per square inch), with 350 representing the highest strength. These steels achieve their strength through precipitation hardening of intermetallic compounds, rather than through carbon content.

 

Comparison with Core Standards

 

Grade Primary AMS Standard Other Key Standards
18Ni250 AMS 6512 MIL-S-46850,UNS K92890,W.Nr. 1.6359
18Ni300 AMS 6514 MIL-S-46850,UNS K93120,W.Nr. 1.6354
18Ni350 AMS 6515 MIL-S-46850,UNS K93160

AMS 6515 has become the primary standard for 18Ni350, covering forms such as bars, forgings, mechanical tubing, and rings, while mandating high purity achieved through double vacuum melting. However, in actual procurement, suppliers may still cite MIL-S-46850 or proprietary standards (such as Vascomax 350) as supplementary references.

 

chemical composition

 

Element 18Ni250 18Ni300 18Ni350
Ni 17 – 19 17 – 19 17.5 – 18.5
Co 7 – 8.5 8.5 – 9.5 12 – 12.5
Mo 4.6 – 5.2 4.6 – 5.2 3.8 – 4.6
Ti 0.3 – 0.5 0.5 – 0.8 1.4 – 1.7
Al 0.05 – 0.15 0.05 – 0.15 0.10 – 0.15
C ≤ 0.03 ≤ 0.03 ≤ 0.03

 

Physical Properties

 

Property Indicator 18Ni250 18Ni300 18Ni350 40HQ
Density (g/cm³) 8.0 8.0 – 8.1 Approx. 8.0 476PCS
Modulus of Elasticity (GPa) 200 190 – 210 Approx. 200 (typical value) 420PCS
Thermal Conductivity (W/m·K) 14 – 25 25.3 Approx. 30 (near room temperature) 336PCS
Coefficient of Linear Expansion (10⁻⁶/K) 10.1 – 10.4 10.1 11.8 (0–100°C) 302PCS
Melting Point (°C) Approx. 1430 – 1450 Approx. 1430 – 1450 Approx. 1390 – 1400 252PCS
Electrical Resistivity (μΩ·m) Approx. 1.1 0.36 – 0.7 --  

 

Comparison of Mechanical Properties (Aged Condition)

 

Property 18Ni250 18Ni300 18Ni350
Tensile Strength ~1790 MPa ~2000 MPa ~2400 MPa
Yield Strength ~1730 MPa ~1900 MPa ~2300 MPa
Elongation ~8–11% ~6–10% ~7–8%
Hardness (HRC) 48–50 51–55 56–59

 

General Processing Guidelines


Cold Working: All three grades exhibit excellent cold workability in the solution-annealed state. They have a very low work-hardening exponent (0.02–0.03), allowing for deformations exceeding 90% without the need for intermediate annealing. This is a key advantage of maraging steels over conventional ultra-high-strength steels.

 

Welding: All three grades possess excellent weldability. Neither preheating nor post-heating is required; direct aging restores over 90% of the joint strength. Welding wire composition must match the base metal (0.5% Ti for grade 250, 0.8% Ti for grade 300, and 1.6% Ti for grade 350).

 

Machining: Rough machining is performed in the solution-annealed state (hardness ~28–30 HRC), with only finish machining required after aging. Dimensional changes during aging are minimal (linear shrinkage of 0.04%–0.08%), allowing for precise tolerance allowances.

 

Surface Treatment: All three grades are suitable for nitriding; the gas nitriding process for 18Ni300 involves treatment at 455°C for 24–28 hours. Due to its high titanium content, careful control of the nitrogen potential is required when nitriding grade 350.

 

 

How to choose?

 

18Ni250
Used for components subject to impact or cyclic loading where failure would have severe consequences-such as rocket motor cases, critical aircraft landing gear parts, and high-pressure vessels. The 250 grade is the preferred choice for safety-critical components or applications involving a risk of impact.

 

18Ni300
Suitable for most load-bearing structural components. Typical applications include steam generator tube-plugging tie rods in nuclear power plants (requiring high yield strength, good fatigue performance, and compact cross-sections), precision injection/die-casting molds (requiring high hardness and impact resistance), as well as satellite structural components and transmission gears. The 300 grade is the standard choice when high strength is required without significantly compromising toughness.

 

18Ni350
Used for components where weight reduction is critical, and the load is primarily static-such as missile/rocket motor cases and aircraft actuator gears. Note that its fatigue strength does not increase in tandem with its tensile strength; therefore, it is unsuitable for applications involving high-cycle cyclic loading.

18Ni250 / 18Ni300 / 18Ni350 Maraging Steel

 

 

Lork Group
Marketing Operations Department
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488

 

Hot Tags: 18Ni250 steel, 18Ni300 steel, 18Ni350 steel, Maraging steel bar, UNS K92890 sheet, UNS K93120 plate, Ni18Co8Mo5Ti, Ni18Co9Mo5Ti,maraging steel, martensitic steel,ASTM A538, A579

Send Inquiry