1J85 Nickel–iron Magnetic Alloy
Ultra-High Permeability – Optimal performance in weak magnetic fields.
Low Core Loss & Near-Zero Magnetostriction – Ensures stability & efficiency.
Custom Solutions – Tailored compositions for specialized applications.
Applications: Magnetic shielding, sensors, transformers, inductors, aerospace components, and more.
in one-stop service
The 1J85 Nickel-Iron Magnetic Alloy (also known as Ni80Mo5, E11c, Permalloy, 79HMA, or PCS) is a high-performance soft magnetic alloy composed of approximately 80% nickel (Ni), 15-20% iron (Fe), and small additions of molybdenum (Mo) and other trace elements.
Widely used in the radio-electronic industry, precision instruments, remote control and automatic control system.

Key Characteristics
High Permeability – Excellent magnetic response in weak magnetic fields.
Low Coercivity – Easily magnetized and demagnetized, reducing energy loss.
Near-Zero Magnetostriction – Minimizes dimensional changes under magnetization, improving stability.
Good Corrosion Resistance – Nickel content provides resistance to oxidation.
chemical composition
|
material |
1J85 |
|||||||
|
chemical composition |
C |
P |
S |
Mn |
Si |
Ni |
Mo |
Cu |
|
≦0.03 |
≦0.02 |
≦0.02 |
0.30-0.60 |
0.15-0.30 |
79.0-81.0 |
4.80-5.20 |
≦0.20 |
|
Mechanical properties
|
Yield strength |
Tensile Strength |
Elongation |
|
Mpa |
Mpa |
% |
|
980 |
1030 |
3~50 |
Physical properties
|
Density (g/cm³) |
8.75 |
|
Electrical resistivity at 20℃(Ωmm2/m) |
0.56 |
|
Coefficient of linear expansion(20℃~200℃)X10-6/℃ |
10.9~11.2 |
|
Saturation magnetostriction coefficient λθ/ 10-6 |
0,5 |
|
Curie point Tc/ ℃ |
400 |
|
The magnetic properties of alloys with high permeability in weak fields |
|||||||
|
1J85 |
Initial permeability |
Maximum permeability |
Coercivity |
Saturation magnetic induction intensity |
|||
|
Сold-rolled strip/ sheet. Thickness, mm |
μ0.08/ (mH/m) |
μm/ (mH/m) |
Hc/ (A/m) |
BS/ T |
|||
|
≥ |
≤ |
||||||
|
0.01 mm |
20 |
87.5 |
4.8 |
0.75 |
|||
|
0.1~0.19 mm |
37.5 |
187.5 |
1.6 |
||||
|
0.2~0.34 mm |
50 |
225 |
1.2 |
||||
|
0.35~1.0 mm |
62.5 |
312.5 |
0.8 |
||||
|
1.1~2.5 mm |
50 |
187.5 |
1.2 |
||||
|
2.6~3.0 mm |
43.8 |
150 |
1.44 |
||||
|
cold drawn wire |
|
||||||
|
0.1 mm |
8.7 |
37.6 |
6.4 |
||||
|
Bar |
|
||||||
|
8-100 mm |
37.5 |
125 |
1.6 |
||||
heat treatment
|
Mode of heat treatment 1J85 |
|
|
Annealing media |
Vacuum with a residual pressure not higher than 0.1Pa, hydrogen with a dew point of not higher than minus 40 ℃. |
|
The heating temperature and rate |
1100~1200℃ |
|
Holding time/h |
3~6 |
|
Cooling rate |
With 100 ~ 200 ℃/ h cooled to 500~600 ℃, not less than 400℃/h cooled to 300℃ |
Application
- Electronics & Telecommunications: Transformer cores, magnetic shielding, inductors.
- Precision Instruments: Sensors, relays, high-accuracy measuring devices.
- Automation & Control Systems: Actuators, magnetic amplifiers.
- Aerospace & Defense: Gyroscopes, navigation systems.
This alloy is crucial in applications requiring minimal hysteresis loss and high magnetic sensitivity, making it a preferred choice in advanced electronics and instrumentation.
Style of supply
|
Alloys Name |
Type |
Dimension |
||
|
1J85 |
Wire |
D= 0.1~8mm |
||
|
1J85 |
Strip |
W= 8~390mm |
T= 0.3mm |
|
|
1J85 |
Foil |
W= 10~100mm |
T= 0.01~0.1 |
|
|
1J85 |
Bar |
Dia= 8~100mm |
L= 50~1000 |
|
Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.