904L Stainless Steel Sheet
Lork Group is 904L Stainless Steel sheet supplier and exporter. 904L (UNS N08904) is a superaustenitic stainless steel designed for corrosion and pitting resistance in a wide range of process environments. It is used extensively in the chemical process industry including the production of phosphate-based fertilizers.
904L Stainless Steel sheet that is designed for moderate to high corrosion resistance in a wide range of process environments. The combination of high chromium and nickel content, coupled with additions of molybdenum and copper, assure good to excellent corrosion resistance.
We keep a selection of common sizes of 904L Stainless Steel sheet in stock. If you have high requirements for the delivery time of the plates, you can confirm with us request a quote.
Specification
|
Dimensions : |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Width: |
1000 MM TO 2500 MM |
|
Thick: |
0.5 MM TO 200 MM |
|
Length: |
100MM TO 600MM |
|
Form : |
Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
|
Finish : |
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
|
Hardness : |
Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
Chemical Composition
|
Element |
Content (%) |
|
Carbon |
0.02% max |
|
Manganese |
2.00% max |
|
Silicon |
1.00% max |
|
Phosphorous |
0.045% max |
|
Sulphur |
0.035% max |
|
Chromium |
19.00-23.00% |
|
Nickel |
23.00-28.00% |
|
Molybdenum |
4.00-5.00% |
|
Copper |
1.00-2.00% |
Mechanical Properties
|
Grade |
Tensile Strength (MPa) min |
Yield Strength 0.2% Proof (MPa) min |
Elongation (% in 50mm) min |
Hardness |
|
|
Rockwell B (HR B) |
Brinell (HB) |
||||
|
904L |
490 |
220 |
36 |
70-90 typical |
150 |
Corrosion Resistance
Where a level of resistance to pitting corrosion better than 316 is required 904L may be suitable. With its high nickel content at 25% it offers improved resistance to chloride stress corrosion cracking compared to other austenitic grades such as 304.
Application
Air Pollution Control - scrubbers for coal-fired power plants
Chemical Processing - process equipment for the production of sulfuric, phosphoric, inorganic and organic acids and the production of phosphate-based fertilizers
Metallurgical Processing - pickling equipment using sulfuric acid
Oil and Gas Production - offshore process equipment
Pharmaceutical Industry - process equipment
Pulp and Paper - processing equipment
Seawater and Brackish Water - condensers, heat exchangers and piping systems
Surface Treatment

Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.
Hot Tags: 904l stainless steel sheet, China 904l stainless steel sheet manufacturers, factory
You Might Also Like
Send Inquiry