Nimonic 86 Nickel Alloy Sheet(UNS N06086)
Nimonic 86 Alloy Sheet is A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. Exhibits good weldability, workability, ductility and creep. Alloy 86 has good formability and weldability with exceptional resistance to oxidation and scaling to 1050°C (1920°F).
Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
65 |
|
Chromium, Cr |
25 |
|
Molybdenum, Mo |
10 |
|
Carbon, C |
0.05 |
|
Cerium, Ce |
0.03 |
Physical Properties
|
Properties |
Metric |
Imperial |
|
Density |
8.54 gm/cm3 |
0.309 lb/in3 |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile strength(annealed) |
825 MPa |
120 ksi |
|
Yield strength(annealed) |
410 MPa |
59 ksi |
|
Elongation at Break |
42% |
42% |
|
Modulus of Elasticity |
210 GPa |
30500 ksi |
Machinability
The conventional machining methods used on iron alloys may be used for this alloy. This alloy work-hardens during machining and exhibits higher strength.
Welding
Nimonic alloy 86 can be welded using common techniques, using a matching filler metal.
Cold working
Cold working may be done on the alloy for hardening.
Annealing
Nimonic alloy 86 should be solution annealed.
Application
The Nimonic 86 Alloy Sheet is used in the following applications:
- Gas turbine engineering
- Industrial furnaces
- Combustion chambers.
Email: susan@lorkgroup.com
WhatsApp: +86 19937075488
Hot Tags: Nimonic 86, Alloy 86, Nickel Alloy Sheet, UNS N06086, W.-Nr. 2.4972, AMS 5910, solid-solution strengthened nickel alloy, high-temperature alloy plate
You Might Also Like
Send Inquiry