Hastelloy C-276 Plate(UNS N10276)
Lork Group is a reliable supplier and exporter of Hastelloy C276 Sheet & Plate in China. With a focus on precision engineering and quality assurance, we delivers reliable solutions for industrial applications, ensuring optimal performance and durability.
Considered one of the most versatile corrosion resistant alloys available, Hastelloy C276 sheet exhibits excellent resistance in a wide variety of chemical process environments including those with ferric and cupric chlorides, hot contaminated organic and inorganic media, chlorine, formic and acetic acids, acetic anhydride, seawater, brine and hypochlorite and chlorine dioxide solutions.
What are the characteristics of Hastelloy C276 Sheet?
- Excellent corrosion resistance in reducing environments
- Exceptional resistance to strong solutions of oxidizing salts, such as ferric and cupric chlorides
- High nickel and molybdenum contents providing good corrosion resistance in reducing environments
- Low carbon content which minimizes grain-boundary carbide precipitation during welding to maintain resistance to corrosion in heat-affected zones of welded joints
- Resistance to localized corrosion such as pitting and stress-corrosion cracking
- One of few materials to withstand the corrosive effects of wet chlorine gas, hypochlorite and chlorine dioxide
We keep a selection of common sizes of Hastelloy C276 Sheet in stock. If you have high requirements for the delivery time of the plates, you can confirm with us.
Specification
|
Dimensions : |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Width: |
1000 MM TO 2500 MM |
|
Thick: |
0.5 MM TO 200 MM |
|
Length: |
100MM TO 600MM |
|
Form : |
Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
|
Finish : |
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
|
Hardness : |
Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
57 |
|
Molybdenum, Mo |
15-17 |
|
Chromium, Cr |
14.5-16.5 |
|
Iron, Fe |
4-7 |
|
Tungsten, W |
3-4.50 |
|
Cobalt, Co |
2.50 |
|
Manganese, Mn |
1 |
|
Vanadium, V |
0.35 |
|
Silicon, Si |
0.080 |
|
Phosphorous, P |
0.025 |
|
Carbon, C |
0.010 |
|
Sulfur, S |
0.010 |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile strength (@thickness 4.80-25.4 mm, 538°C/@thickness 0.189-1.00 in, 1000°F) |
601.2 MPa |
87200 psi |
|
Yield strength (0.2% offset, @thickness 2.40 mm, 427°C/@thickness 0.0945 in, 801°F) |
204.8 MPa |
29700 psi |
|
Elastic modulus (RT) |
205 GPa |
29700 ksi |
|
Elongation at break (in 50.8 mm, @thickness 1.60-4.70 mm, 204°C/@thickness 0.0630-0.185 in, 399°F) |
56% |
56% |
|
Hardness, Rockwell B (plate) |
87 |
87 |
Application
Hastelloy C276 is used for rotors, bolts, shafts, blades and other components in marine applications and other industries, including pollution control; food, waste and chemical processing; paper operations; and multipurpose plants.
Tungsten has been added to this versatile nickel-chromium-molybdenum alloy, which resists crevice corrosion, stress corrosion cracking, and pitting. Resistant to chloride ions and sulfur blends, Hastelloy C276 is ideal for flue gas desulfurization applications.