MP159 Cobalt Alloy Rod Sent to South Korea

Jun 20, 2024

Leave a message

On June 19, we supplied a batch of high quality MP159 Cobalt alloy rod to our Korean customer. They have high dimensional requirements and mechanical performance requirements for materials. In the end, the customer was very satisfied with the entire shipment.

 

Customers have requirements for the properties of this batch of materials.MP159 is from the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility, and corrosion resistance.

 

MP159 alloy bars

 

Through work strengthening and aging, MP159 exhibits ultimate tensile strength levels in excess of 265,000 psi while maintaining reduction of area values greater than 30%. Excellent strength and ductility are also evident at elevated temperatures up to 1100 - 1200 °F (593-649°C). It is produced by vacuum induction melting followed by VAC-ARC remelting to provide optimum control of chemistry and preferred ingot solidification.

 

With so many requirements, customers naturally have certain concerns about the performance of materials. They asked to provide a sample for them to test the properties and dimensions of the material before shipping. And precisely because we have full confidence in the material, we are happy to provide samples.

 

Finally, the sample passed the test. The customer is satisfied with the entire order.