  Congratulations to Lork Group on reaching a cooperation agreement with a Mexican customer for the delivery of Inconel 718 mold nickel alloy. Our goods have been produced, tested, and packaged. The relevant production test reports have been sent back to the customer. We are waiting for the customer's freight forwarder to transport them. Lork Group has efficiently completed this Inconel 718 mold nickel alloy order!

 

what is Inonel 718 Nickel Alloy?

Lork Group supplies Inconel 718 , a precipitation-hardening nickel-chromium alloy known for its high strength, corrosion resistance, and ability to maintain these properties at high temperatures. This type of nickel alloy is widely used in aerospace, petrochemical, and other fields.

 

Inconel 718 Key Characteristics:

Corrosion and Oxidation Resistance

Weldability and Formability

High-Temperature Performance

Inconel 718

High quality

quick delivery for our globad istributors

advanced equipment

Forging die processing and manufacturing

professional team

A smooth experience from inquiry to delivery

one-stop solution

Customized comprehensive solutions

 

Inconel 718 Nickel Alloy Mold Technical Data Sheet

 

Nickel Alloy 718/ Inconel 718/Werkstoff Nr 2.4668

 

 
 

Inconel 718 Chemical Composition Limits

C

0.10 max

MN

0.50 max

P

0.15 max

S

.015 max

Si

.50 max

Cr

20.0 -23.0

Ni

58.0 min

Mo

8.0- 10.0

Co

1.0 max

Ti

0.40 max

Al

0.40 max

Fe

5.0 max

NB

3.15- 4.15

 

Inconel 718 Nickel Alloy Typical Mechanical Properties

 

There are two main types of solution annealed and aging treatments:
1)
Solution Treatment (AMS 5662 Bar / AMS 5596 Sheet): 1725°F - 1850°F + Air Cool.
Heat Treatment (AMS 5663 Bar) : 1325°F for 8 hrs, cooling 100°F/hr to 1150°F, hold at 1150°F for 8hrs min, + Air Cool .

This treatment gives the highest room temperature tensile and yield strengths as well as producing the highest fatigue strength. It is the optimum heat treatment for Alloy 718 where a combination of rupture life, notch rupture life and rupture ductility is required.

2)
Alternative Solution Treatment (AMS 5664 Bar / AMS 5597 Sheet): 1900°F - 1950°F + Air Cool
Heat Treatment: 1400°F for 10hrs, furnace cool to 1200°F, hold at 1200°F for a total aging time of 20 hrs + Air Cool.

This is the prefered treatment in tensile-limited applications as it produces the best transverse ductility in heavy sections, impact strength and low temperature notch tensile strength. However, this treatment has a tendency to produce notch brittleness in stress rupture.

 

Inconel 718 nickel alloy stock specifications available at Lork Group

 

To learn more about the inventory status of different materials, please contact us!

 

Grade Inconel 718/ Nickel Alloy
Nickel plate Thickness: 0.3mm - 150.0mm
Width: 1000mm - 3000mm
Nickel bar Diameter: Ф4mm - Ф600mm
Nickel coil Thickness: 0.3mm - 16.0mm
Width: 1000mm - 3000mm
Nickel pipe Outside diameter: 6mm - 1219mm
Thickness: 0.5mm - 100mm

 

modular-1

One-stop Nickel Alloy in China

If you are interested in nickel alloy materials, you can discuss with us.

 

Send Inquiry