Monel k500
Lork Group specializes in supplying Monel K500 bars, pipes, plates, and strips. For more product information, please click the image link below to view the details.
Details
Lork Group high-quality Monel K500 (UNS N05500/ W. Nr. 2.4375) is a nickel-copper alloy, precipitation-hardened through additions of aluminum and titanium.
To obtain a quote or size specifications, please contact:
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488
Products Description
Lork Group high-quality Monel K500 (UNS N05500/ W. Nr. 2.4375) is a nickel-copper alloy, precipitation-hardened through additions of aluminum and titanium. MONEL K500 retains the excellent corrosion-resistant characteristics of 400 and has enhanced strength and hardness after precipitation hardening when compared with 400.
Product Form
Bar, forging: AMS 4676, ASTM B865
Pipe and Tube: DIN 17751
Plate, Sheet, and Strip: DIN 17750
Monel K500 Chemical Composition
|
Composition |
Content(%) |
|
|
Min |
Max |
|
|
Ni |
63 |
|
|
Cu |
27.0 |
33.0 |
|
Al |
2.30 |
3.15 |
|
Ti |
0.35 |
0.85 |
|
Fe |
2.0 |
|
|
Mn |
1.5 |
|
|
S |
0.01 |
|
|
C |
0.25 |
|
|
Si |
0.5 |
|
Monel K500 Property
|
Tensile Strength (σb/MPa) |
Yield Strength (σp0.2/MPa) |
Elongation (σ5/%) |
|
1100 |
790 |
20 |
Monel K500 Application
Typical applications for this nickel-copper superalloy and its products are turbine blades and gas turbine blades for aircraft engines, fasteners and springs for marine services, pump and valve components for chemical processing, doctor blades and scrapers for pulp processing in paper production, etc.
- Chemical Industry (valves and pumps)
- Paper Production (doctor blades and scrapers)
- Oil and Gas (pump shafts, drill collars and instruments, impellers, and valves)
- Electronic components and sensors
Monel K500 Characteristics
Virtually nonmagnetic, even at quite low temperatures
Exceptionally good dimensional stability
Resistant to a sour-gas environment
Excellent corrosion resistance together with increased strength and hardness over that of Alloy 400