Inconel 600

Lork Group specializes in supplying bars, tubes, plates, strips, and custom-machined parts. For more product details, please click the image below to visit the link.

Inconel 600 Nickel Alloy Bar (UNS N06600)
Inconel 600 Nickel Alloy Tube (UNS N06600)
Inconel 600 Sheet
ASTM B168 Inconel 600 Strip
Premium Inconel 600 Spring Manufacturer

Details

 

Lork Group's high-quality Inconel 600 offers exceptional resistance to high-temperature corrosion and oxidation, making it a versatile material for medium-to-high temperature environments and moderately corrosive conditions.

Need a quote or dimensional information? Feel free to contact us anytime!
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Inconel 600(UNS N06600/W.Nr. 2.4816) is a nickel-chromium alloy renowned for its exceptional resistance to high-temperature corrosion and oxidation.

Primarily nickel-based, with significant chromium additions, it delivers outstanding mechanical properties at elevated temperatures, making it a popular choice for extreme-environment applications.

Its high nickel content provides excellent resistance to chloride-ion stress-corrosion cracking, while its chromium component contributes to its resistance to sulfur compounds and oxidizing conditions.

 

Product Form

 

Bar: ASTM B 473

Plate/Sheet/Strip: ASME SB-463, ASME SB-464, ASTM B 463, ASTM B464

Wire: ASME SB-473, ASME SB-366, ASTM B 473, ASTM B 366

Pipe: ASTM B464

 

Inconel 600 Chemical Composition

 

Inconel 600

Content (%)

Min

Max

Ni

72

 

Cr

14

17

Fe

6

10

C

 

0.15

Mn

 

1

Si

 

0.5

Cu

 

0.5

P

 

0.015

S

 

0.015

 

Inconel 600 Property

 

Material

Form and Condition

Tensile Strength

Yield Strength

Elongation %

Hardness, Rockwell

ksi

MPa

ksi

MPa

Alloy 600 rod and bar

Cold drawn Annealed

80-100

550-690

25-50

170-345

55-35

65-85B

Alloy 600 Plate

Hot rolled Annealed

80-100

550-725

30-50

205-345

55-35

65-85B

Alloy 600 Sheet

Cold Rolled Annealed

80-100

550-690

30-45

205-310

55-35

88B max

Alloy 600 Tube & Pipe

Cold Drawn Annealed

80-100

550-690

25-50

170-345

55-35

88B max

Alloy 600 Wire

Cold Drawn Annealed

80-120

550-830

35-75

240-520

45-20

-

Alloy 600 Wire

Cold Drawn No 1 Temper

105-135

725-930

70-105

480-725

35-15

-

Alloy 600 Wire

Spring Temper

170-220

1170-1520

150-210

1035-1450

5-2

-

 

Inconel 600 Key Performance

 

  • High-Temperature Strength:Demonstrating remarkable strength and stability at elevated temperatures, Alloy 600 retains its mechanical properties even in extreme environments, making it well-suited for high-temperature applications.
  • Corrosion Resistance:Alloy 600 boasts excellent corrosion resistance, including resistance to chloride-ion stress corrosion cracking, oxidation, and scaling at high temperatures. This property ensures the longevity and reliability of equipment made from Alloy 600.
  • Thermal Expansion:The low thermal expansion coefficient of Alloy 600 allows it to maintain dimensional stability under varying temperature conditions. This characteristic is crucial in applications where dimensional integrity is essential.
  • Electrical Conductivity:Alloy 600 exhibits good electrical conductivity, making it suitable for electrical resistance heating elements and thermocouples. Its electrical properties contribute to its effectiveness in various industrial applications.

 

Inconel 600 Application

 

  • Nuclear reactor vessels and heat exchanger tubing
  • Chemical processing equipment
  • Heat treat furnace components and fixtures
  • Gas turbine components including jet engines
  • Electronic parts

 

Inconel 600 finds extensive use in industries such as aerospace, chemical processing, and nuclear engineering, where it is employed in applications ranging from furnace components and heat-treating equipment to chemical processing vessels and gas turbine components. Its ability to maintain strength and resist deformation at high temperatures, along with its excellent resistance to oxidation and carburization, make it a valuable material for demanding environments.

Furthermore, Inconel 600 offers good weldability and high thermal stability, allowing for ease of fabrication and forming. Its combination of high strength, corrosion resistance, and fabricability makes it a versatile and reliable material for a wide range of challenging applications, earning it a reputation as a high-performance alloy in demanding industrial settings.

 

Send Inquiry Now