Hastelloy G30

One-stop supply of Hastelloy G30 bars, pipes, plates, and strips. Want to know more? Click the image below to view details.

Hastelloy G30 Alloy Bar
Hastelloy G-30 Pipe(UNS N06030)
Hastelloy G-30 Nickel Sheet(UNS N06030)
Hastelloy G-30 Strip
page-600-600

Details

 

Lork Group's high-quality Hastelloy G30 is a highly corrosion-resistant nickel-base alloy designed for service in harsh environments involving strong oxidizing acids.

Want the latest quotes and dimensions? Contact us today!
 layla@lorkgroup.com |  +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Hastelloy G30 is a highly corrosion-resistant nickel-base alloy designed for service in harsh environments involving strong oxidizing acids. Developed as an improvement over earlier Hastelloy alloys, G30 offers exceptional resistance to a wide range of chemical environments, including nitric acid, phosphoric acid, hydrochloric acid, sulfuric acid, and various mixtures thereof.

 

Product Form

 

Rod, Bar, Wire and Forgings: ASTM B462, ASTM B581, ASME SB462, ASME SB581

Plate, Sheet and Strip: ASTM B575, ASME SB575

Pipe and Tube: ASTM B619, ASTM B622, ASTM B626, ASME SB619, ASME SB622, ASME SB626

Welding Product: AWS A5.14 ERNiCrMo-11, ASME Ⅱ SFA-5.14 ERNiCrMo-11, ASME Ⅸ F-No.45

Forgings

 

Hastelloy G30 Chemical Composition

 

Composition

Content

C

≤0.03

Si

≤0.80

Mn

≤1.50

P

≤0.04

S

≤0.03

Cr

28.0-31.5

Ni

Bal

Co

≤5.00

Mo

4.0-6.0

W

1.5-4.0

Nb+Ta

0.3-1.5

Cu

1.0-2.4

Fe

13.0-17.0

 

Hastelloy G30 Property

 

Density, g/cm3

Melting Point, ℃

Tensile Strength, MPa

Yield Strength, MPa

ELongation, %

Hardness, HB

8.14

1260-1343

690

321

50

–

 

Hastelloy G30 Application

 

  • Phosphoric Acid Service
  • Sulfuric Acid Service
  • Nitric Acid Service
  • Nuclear Fuel Reprocessing
  • Nuclear Waste Processing
  • Pickling Operations
  • Petrochemicals
  • Fertilizer Manufacture
  • Pesticide Manufacture
  • Gold Ore Extraction

 

Key features of Hastelloy G30 include

 

Excellent Corrosion Resistance: It provides superior resistance to both oxidizing and reducing acids, as well as resistance to localized corrosion such as pitting and crevice corrosion.

High Strength: Hastelloy G30 maintains its mechanical properties at elevated temperatures, making it suitable for applications where both corrosion resistance and structural integrity are crucial.

Fabricability: The alloy is easily formed, welded, and machined, allowing for versatile manufacturing processes and ease of maintenance.

The composition of Hastelloy G30 typically includes high levels of chromium, nickel, and molybdenum, along with additions of tungsten and cobalt, which collectively enhance its resistance to corrosion and maintain its mechanical strength in demanding conditions.

 

 