Udimet 720 Nickel Alloy

Udimet 720 Nickel Alloy

Lork Group offers Udimet 720 nickel alloy, which is available for third-party testing and custom fabrication in a variety of specifications. Inquire online!
Send Inquiry

Welcome to Lork Group, your nickel Alloy manufacturer and exporter.

 

Udimet 720 nickel alloy utilizes a solid solution strengthening process with tungsten and molybdenum, combined with precipitation hardening metallurgy with titanium and aluminum to achieve a qualified chemical composition.

 

Please provide your desired Udimet 720 nickel alloy specifications, quantity, and application to Email: susan@lorkgroup.com/WhatsApp: +86 19937075488, so that we can provide you with a quick quote.


What are the characteristics of Udimet 720 nickel alloy?


1. High strength and metallurgical stability
2. Excellent impact strength retention and long-term high temperature resistance
3. Excellent oxidation and sulfur corrosion resistance
4. Excellent fatigue and creep resistance.

 

If you are interested in Udimet 720 nickel alloy, please click the circle icon below to initiate an online communication.

 

Nickel Alloy Udimet 720 parameters

 

 Udimet 720 Nickel Alloy stock

Lork Group is rooted in "Global Craftsmanship, Intelligent Manufacturing in China," with full-process quality control as the core, and rigorously selected suppliers. We professionally craft nickel alloys for you!.
Udimet 720 rod

Udimet 720 Bar

Specifications

 
Udimet 720 sheet

Udimet 720 Plate

Specifications

 
Udimet 720 tube

Udimet 720 Pipe

Specifications

 
Udimet 720 strip

Udimet 720 Strip

Specifications

 

Udimet 720 Manufacturing Process and Challenges

 

      Welding and Processing :Udimet alloy 720 offers good weldability and processing characteristics:

      Welding: Can be welded using methods such as TIG, MIG, and resistance welding. Preheating and post-weld heat treatment may be required to maintain properties.

     Machinability: Generally machined in the solution-annealed condition using carbide tools and appropriate cutting fluids.

     Lork Group offers customized Udimet 720 nickel alloy in various specifications for applications in aerospace, medical, oil and gas, and other industries. We have successful client collaborations.
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

Udimet 720 LorkGroup

Udimet 720 Nickel Alloy Chemical Composition

Weight% Alloy 901
Ni 55.16-59.70
Cr 15.5-16.5
Mo 2.75-3.25
Ti 4.75-5.25
Co 14.0-15.5
W 1.00-1.50
Zr/B/C Trace

Udimet 720 Nickel Alloy Mechanical Properties

Material Udimet 720
Tensile Strength ksi 170 – 190 (1172 – 1310)
Yield Strength ksi 120 – 140 (827 – 965)
Elongation (% in 2 inches) 15 – 20
Hardness HB 35 – 40

 For more information on Udimet 720 Nickel Alloy, please contact us.

 

Contact now

 

 

Metal Sample Testing by Lork Group

Lork Group Spectrometer Testing

Lork Group Packaging

 

 

Lork Group Company Introduction

 

Hot Tags: udimet 720 nickel alloy, China udimet 720 nickel alloy manufacturers, factory

Send Inquiry