AMS 5715 / UNS N06601 / Inconel 601 Nickel Bar
AMS 5715 specifies the requirements for Inconel 601 (UNS N06601), a nickel-chromium-iron alloy designed for extreme heat and corrosion resistance. This standard covers bars, forgings, flash-welded rings, and stock used in high-performance industrial applications.
Inconel 601 is renowned for its exceptional oxidation resistance up to 2200°F (1204°C), making it ideal for welded components, furnace parts, and chemical processing equipment. Its balanced composition ensures long-term durability in aggressive environments, including exposure to sulfuric acid, nitric acid, and other corrosive media.
Industries & Applications
01
Aerospace & Jet Engines
Combustor liners, afterburner components, and exhaust systems.
02
Thermal Processing & Furnace Systems
Radiant tubes, muffles, and heat-treating baskets.
03
Chemical & Petrochemical Processing
Reactor vessels, catalyst grids, and piping in corrosive environments.
04
Power Generation & Pollution Control
Heat recovery systems, boiler components, and flue gas desulfurization units.
Chemical Composition
| Weight% | Ni | Cr | Fe | Al | C | Mn | S | Si | C |
| Alloy 601 | 58-63 | 21-25 | Rem | 1-1.7 | 0.10 max | 1.0 max | 0.015 max | 0.50 max | 1.0 max |
Mechanical Properties
| Material | Form and Condition | Tensile Strength | Yield Strength | Elongation % | Hardness, HB | ||
| ksi | MPa | ksi | MPa | ||||
| Inconel 601 Bar | Bar Annealed | 80-115 | 550-790 | 30-60 | 205-415 | 70-40 | 60-80 |
| Inconel 601 Sheet | Sheet Annealed | 85-100 | 585-690 | 30-50 | 205-345 | 55-35 | 65-80 |
| Inconel 601 Plate | Plate Annealed | 80-100 | 550-690 | 30-45 | 205-310 | 65-45 | 60-75 |
Inconel 601 can withstand corrosion and oxidation resistance of up to 2200°F (1204°C). This makes it an excellent choice for parts that require welding during fabrication, as well as for parts that will be used in harsh environments, such as those exposed to corrosives.
The annealing process is suitable for tensile-limited applications at temperatures below 1000°F (540°C), whereas solution heat treatment designations apply to rupture-limited applications at temperatures exceeding 1000°F (540°C).
Lork Group is a leading global supplier of high-quality Inconel 601 Nickel Bars compliant with AMS 5715/UNS N06601 specifications. We provide premium-grade alloy 601 bars, forgings, and flash-welded rings for the most demanding high-temperature applications.
Why Choose Lork Group for Your Inconel 601 Needs?
- Superior Material Properties - Our Inconel 601 offers exceptional oxidation resistance up to 2200°F (1204°C) and excellent corrosion resistance in harsh environments
- AMS 5715 Certified - All materials meet strict aerospace material specifications for bars, forgings, and welded components
- Multiple Processing Options - Available in annealed or solution-treated conditions for optimal performance in your specific temperature range
- Global Supply Network - Reliable worldwide logistics with competitive lead times
- Technical Expertise - Our metallurgical specialists can help select the right grade and treatment for your application
Request Your Quote Today!
Contact Lork Group for:
- Current Inconel 601 inventory availability
- Competitive pricing for bulk orders
- Complete material certifications
- Technical specifications and processing recommendations
Hot Tags: ams 5715 / uns n06601 / inconel 601 nickel bar, China ams 5715 / uns n06601 / inconel 601 nickel bar manufacturers, factory
You Might Also Like
Send Inquiry