Incoloy 945 Nickel Alloy (UNS N09945, API 6ACRA)
API 6A CRA Incoloy 945 Nickel Alloy Nickel Alloy Description
Incoloy 945 is a nickel-iron-chromium precipitation hardening alloy specially designed for oil and gas fields that is resistant to acid corrosion. The general supply and production standards are API 6A CRA (oil and gas field equipment) and the commonly used ASTM B804 standard.
API 6A CAR Incoloy 945 Nickel Alloy purchasing tips:
1. Clarify standards and certifications:
When purchasing, ensure that the material complies with relevant standards (such as API 6A CRA) and request a complete material certificate. It also complies with NACE MR0175/ISO 15156 standards.
2. Focus on smelting and heat treatment:
Based on your processing and end-use requirements, clarify the heat treatment state of Incoloy 945 nickel alloy (e.g., solution state, aged state), as this is critical to the performance of the finished product. Look for suppliers who mention advanced processes such as vacuum melting.
Send us your requirements and contact information to get real-time quotes!
API 6A CRA Incoloy 945 Nickel Alloy Parameters
Incoloy 945 Nickel Alloy Custom
Incoloy 945 Nickel Alloy Manufacturing and Pricing Reference
Incoloy 945 Nickel Alloy bar
Heat Treatment:
This is crucial for achieving optimal properties. A precipitation hardening process, typically solution treating followed by aging, is employed. Aging precipitates γ' and γ'' phases, imparting high strength to the alloy.
Weldability:
The alloy exhibits excellent weldability and can be welded using conventional methods such as TIG (tungsten inert gas) and MIG (metal inert gas). The welded joints exhibit strength and corrosion resistance close to that of the parent metal.
Lork Group offers customized API 6A CRA Incoloy 945 Nickel Alloy. The approximate prices offered by Lork Group are:
1. Stock Material: $40-60/kg (MOQ 30kg), $35-40/kg (100-300kg)
2. Processing: Cutting, chipping, milling, etc. (Price based on material loss and processing method)
For more information, please contact:
Email: susan@lorkgroup.com
WhatsApp: +86 19937075488

The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information!
Incoloy 945 Nickel Alloy Chemical Composition
| Weight% | Incoloy 945 | |
| Mn | ≤ 1.0 | |
| Cr | 19.5 - 23.0 | |
| Mo |
|
|
| Ti | 0.5 - 2.5 | |
| Fe | Bal | |
| Nb | 2.5 - 4.5 | |
| Cu/Si/Al/C/S | Trace | |
| Ni | 45.0 - 55.0 |
Incoloy 945 Nickel Alloy Mechanical Properties
| Material | Incoloy 945 |
| Tensile Strength | ≥ 830 MPa |
| Yield Strength | ≥ 690 MPa |
| Reduction of Area % | ≥ 28% |
| Hardness HBW | ≤ 205 HBW |
For more Incoloy 945 Nickel Alloy details, please contact us!