Haynes 556 Alloy Sheet

Haynes 556 Alloy Sheet

Haynes 556 Alloy Sheet (UNS R30556) is an iron-nickel-chromium-cobalt alloy that combines effective resistance to sulfidizing, carburizing and chlorine-bearing environments at high temperatures with good oxidation resistance
Send Inquiry

Haynes 556 Alloy Sheet (UNS R30556) is an iron-nickel-chromium-cobalt alloy that combines effective resistance to sulfidizing, carburizing and chlorine-bearing environments at high temperatures with good oxidation resistance, fabricability, and excellent high-temperature strength. It has also been found to resist corrosion by molten chloride salts and other salts, and is resistant to corrosion from molten zinc.

 

Haynes 556 Alloy Sheet has excellent forming and welding characteristics. It may be forged or otherwise hot-worked, providing that it is held at 2150°F (1175°C) for a time sufficient to bring the entire piece to temperature. As a consequence of its good ductility, Alloy 556 is also readily formed by cold working. All hot- or cold-worked parts should be annealed and rapidly cooled in order to restore the best balance of properties.

 

Haynes 556 Alloy Sheet can be welded by a variety of techniques, including gas tungsten arc (GTAW), gas metal arc (GMAW), shielded metal arc (coated electrode), and resistance welding.

 

Chemical Composition

 

Element

Content (%)

Iron

31 Balance

Nickel

20

Cobalt

18

Chromium

22

Molybdenum

3

Tungsten

2.5

Tantalum

0.6

Nitrogen

0.2

Silicon

0.4

Niobium

0.3 max.

Manganese

1

Aluminum

0.2

Carbon

0.1

Boron

0.02 max.

Lanthanum

0.02

Zirconium

0.02

 

Heat Treatment

 

Haynes 556 Alloy Sheet is furnished in the solution heat treated condition, unless otherwise specified. The alloy is normally solution heat treated at 2150°F (1175°C) and rapidly cooled or water-quenched for optimum properties. Heat treatments at temperatures lower than the solution heat-treating temperature may cause precipitation of secondary phases.

 

Application

 

  • Incinerators
  • Gas turbines
  • Heat transfer systems

 

 

Manufacturing Process

 

product-1200-682

 

Main Applications

 

product-1200-833

 

Packaging & Shipping

 

product-1200-690

product-1200-1147

 

FAQS

 

If you have any other questions, please contact me!

 

Q: Can you produce nickel alloy bars?

A: Yes, we can produce nickel alloy bars according to your requirements.

Q: What is your minimum order quantity?

A: Our minimum order quantity is 50 kg. Larger quantity, lower price.

Q: How long is your delivery time?

A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.

Q: Can you provide samples?

A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.

Q: How can l quickly get the price list?

A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.

Q: How do you control product quality?

A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.

Q: Can you provide processing services?

A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.

 

 

 

 

 

 

 

Hot Tags: haynes 556 alloy sheet, China haynes 556 alloy sheet manufacturers, factory

Send Inquiry