Hastelloy C22 Wire(UNS N06022)
Hastelloy C22 Wire(UNS N06022)
Hastelloy C22 wire (UNS N06022) is a nickel-chromium-molybdenum-tungsten alloy wire known for its excellent corrosion resistance in a variety of harsh environments. It is particularly good at resisting pitting, crevice corrosion, and stress corrosion cracking. It has excellent resistance to both oxidizing and reducing media, including wet chlorine, nitric acid, and mixed acids containing chlorides. Can be used in the chemical/petrochemical sectors and flue gas desulfurization systems.
Implementation standards: ASTM B574, AWS A5.14, NACE MR0175 (ISO 15156-3).
Typical grades: UNS N06022, W.Nr. 2.4602
Supply Forms and Dimensions
Size range: Diameters from 0.025 mm to 21 mm; a wide range of specifications available.
Supply forms: Available in coils, spools, and straight lengths.
Typical advantages

01
Comprehensive corrosion resistance
Its overall corrosion resistance is superior to that of C-276, C-4, and Inconel 625 alloys. It offers greater adaptability and a lower risk of failure.
02
Local corrosion resistance
C-22 welding wire exhibits excellent resistance to pitting, crevice corrosion, and stress corrosion cracking. In environments containing high concentrations of chlorides or sulfides, it effectively prevents premature material failure caused by localized corrosion.
03
Process adaptability
Effectively prevents the formation of grain boundary precipitates. When used in the post-weld condition, it also maintains good corrosion resistance and performance without requiring complex heat treatments. Good ductility and formability; easy to process into various complex wire products; strong adaptability.
04
Stability over a wide temperature range
It maintains stable performance across an extreme temperature range of -200°C to +400°C, making it suitable for demanding operating conditions such as cryogenic and high-temperature environments. It is available in annealed or spring-tempered conditions as required.
Typical applications
Based on its performance characteristics, C22 wire is commonly used in:

Springs, fasteners, seals




chemical composition
| Nickel | 56 Balance |
| Chromium | 22 |
| Molybdenum | 13 |
| Iron | 3 |
| Cobalt | 2.5 max. |
| Tungsten | 3 |
| Manganese | 0.5 max. |
| Silicon | 0.08 max. |
| Carbon | 0.01 max. |
| Vanadium | 0.35 max. |
| Copper | 0.5 max. |
Physical Properties(RT)
Density:8.69 g/cm3
Electrical Resistivity:1.14 µohm.m
Dynamic Modulus of Elasticity:206 GPa
Melting Range:1357-1399°C
Tensile strength range in the as-supplied condition
| Supply Condition | Tensile Strength (MPa) | Characteristics |
| Annealed | 758 – 1100 | As-supplied condition; good ductility, facilitating subsequent cold forming |
| Spring-tempered | 1379 – 1700 | Strengthened via cold working to achieve ultra-high strength. |
Lork Group
Marketing Operations Department
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488
Hot Tags: Hastelloy C22 Wire,UNS N06022,W.Nr. 2.4602, ASTM B574,Ni-Cr-Mo-W Alloy,Hastelloy C22 wire supplier,C22 Alloy Wire
You Might Also Like
Send Inquiry