Lork Group's high-quality Monel 404 (UNS N04404 / W.Nr. 2.4867) is a nickel-copper alloy that is used primarily in electrical and electronic applications.

Please get in touch with us for product pricing and specifications.
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Monel 404 (UNS N04404 / W.Nr. 2.4867) is a nickel-copper alloy that is used primarily in electrical and electronic applications.

Monel 404 has a relatively high copper content; hence, it is suitable for electrical and electronic applications.

Similar to Monel 401, the chemical composition of Monel 404 is carefully adjusted to provide a very low Curie temperature, low permeability, and good brazing characteristics. Monel 404 has low magnetic permeability and a low Curie temperature.

 

Product Form

 

Rod, Bar, Wire and Forgings: ASTM B164, ASME SB164, DIN 17752

Plate, Sheet and Strip: DIN 17750

Pipe and Tube: DIN 17751

 

Monel 404 Chemical Composition

 

Element

Content (%)

Nickel, Ni

50 - 57 max

Copper, Cu

≤ 45.5

Iron, Fe

≤ 0.50

Carbon, C

≤ 0.15

Manganese, Mn

≤ 0.10

Silicon, Si

≤ 0.10

Aluminum, Al

≤ 0.050

Sulfur, S

0.024

 

Monel 404 Property

 

Density, g/cm3

Melting Point, ℃

Tensile Strength, MPa

Yield Strength, MPa

Elongation, %

Hardness, HRB

8.91

1300-1350

550

185

36

/

 

Monel 404 Application

 