Monel 400
Lork Group offers Monel 400 pipes, plates, strips, and machined parts. Want to learn more? Click the image below for details.
Details
Lork Group high-quality Monel 400 (UNS N04400/. W.Nr. 2.4360 and 2.4361) is a nickel-copper alloy (about 67% Ni – 23% Cu) that is resistant to seawater and steam at high temperatures as well as to salt and caustic solutions.
Need a quote or dimensions? Feel free to contact us anytime!
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488
Products Description
Lork Group high-quality Monel 400 (UNS N04400/. W.Nr. 2.4360 and 2.4361) is a nickel-copper alloy (about 67% Ni – 23% Cu) that is resistant to seawater and steam at high temperatures as well as to salt and caustic solutions. Monel 400 is a solid solution alloy that can only be hardened by cold working.
Monel 400 nickel alloy exhibits characteristics like good corrosion resistance, good weldability, and high strength. A low corrosion rate in rapidly flowing brackish water or seawater, combined with excellent resistance to stress-corrosion cracking in most fresh waters, and its resistance to a variety of corrosive conditions led to its wide use in marine applications and other non-oxidizing chloride solutions.
Monel 400 nickel alloy is particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated. As would be expected from its high copper content, Monel 400 is rapidly attacked by nitric acid and ammonia systems.
Monel 400 has great mechanical properties at subzero temperatures, can be used at temperatures up to 1000° F, and its melting point is 2370-2460° F. However, Monel 400 is low in strength in the annealed condition, so a variety of tempers may be used to increase the strength.
Product Form
Sheet/Plate/Strip: ASTM B127, AMS 4544
Forging: ASTM B564, DIN 17752, AMS 4675
Bar: ASTM B164, DIN 17752, AMS 4675
Tube: ASTM B165, AMS 4574, AMS 4575
Pipe: ASTM B 185
Monel 400 Chemical Composition
|
Composition |
Content |
|
C |
0.3 max |
|
Mn |
2.0 max |
|
S |
0.24 max |
|
Si |
0.5 max |
|
Ni |
63 min |
|
Cu |
28-34 |
|
Fe |
2.5 max |
Monel 400 Property
|
Form |
Condition |
Tensile (Ksi) |
0.2% Yield (Ksi) |
Elongation % |
Hardness (HRB) |
|
Bar |
Annealed |
75-90 |
25-50 |
60-35 |
60-80 |
|
Bar |
Cold drawn |
84-120 |
55-100 |
40-22 |
20-85 |
|
Plate |
Annealed |
70-85 |
28-50 |
50-35 |
60-76 |
|
Sheet |
Annealed |
70-85 |
30-45 |
45-35 |
65-80 |
|
Pipe |
Annealed |
70-85 |
25-45 |
50-35 |
75 max |
Monel 400 Application
- Marine engineering
- Chemical and hydrocarbon processing equipment
- Gasoline and freshwater tanks
- Crude petroleum stills
- De-aerating heaters
- Boiler feed water heaters and other heat exchangers
- Valves, pumps, shafts, fittings, and fasteners
- Industrial heat exchangers
- Chlorinated solvents
- Crude oil distillation towers