Inconel 602CA

Lork Group supplies Inconel 602CA bars; click the image below for details.

Inconel 602CA Alloy Bar
page-600-600
page-800-800
page-600-600
page-600-600

Details

 

Lork Group high-quality Inconel 602CA (UNS N06025 / W.Nr. 2.4633) is the most oxidation resistant,high strength nickel alloy available. It is normally supplied in the solution-annealed condition with an oxidized or descaled surface.

Need a quote or dimensional information? Feel free to contact us anytime!
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group high-quality Inconel 602CA (UNS N06025 / W.Nr. 2.4633) is the most oxidation-resistant, high strength nickel alloy available. Alloy 602 CA is a high-carbon nickel-chromium-iron alloy with additions of the micro-alloying elements titanium and zirconium together with aluminum and yttrium. It is normally supplied in the solution-annealed condition with an oxidized or descaled surface.

 

Characteristic

 

  • Outstanding resistance to cyclic oxidation through 2250°F (1232°C)
  • Excellent high-temperature creep strength
  • Resistant to carburizing and nitriding environments
  • Highly resistant to grain growth in service
  • Superior behavior in oxidizing/chloridizing environments
  • Good resistance to metal dusting

 

Product Form

 

Bar, Forgings, Rings: ASTM B166

Sheet, Plate, Strip: ASTM B168

Pipe, Tube: ASTM B167, ASTM B751, ASTM B775, ASTM B829

 

Chemical Composition

 

Elements

Content (%)

C

0.15-0.25

Si

≤0.50

Mn

≤0.50

P

≤0.020

S

≤0.010

Cr

24.0-26.0

Ni

Bal

AI

1.8-2.4

Ti

0.1-0.2

Cu

≤0.10

Y

0.05-0.12

Zr

0.01-0.10

Fe

8.0-11.0

 

Physical Properties

 

Density

g/cm3

7.93

lb/in.3

0.29

Melting Range

°F

2444 - 2552

°C

1340 - 1400

 

Mechanical Properties

 

Condition & Size

Tensile Strength

Yield Strength
(0.2% Offset)

Elongation

Reduction of Area

Hardness

MPa, min

MPa, min

%, min

%, min

Rockwell

Seamless Pipe & Tube

Hot-worked annealed or cold-worked annealed (all sizes)

680

270

30

...

...

Rod & Bar

Hot-worked annealed or cold-worked annealed (all sizes)

680

270

30

...

...

Plate, Sheet & Strip

Annealed

680

270

30

...

...

 

Applications

 

  • Radiant tubes
  • Furnace muffles
  • Rotary and shaft furnaces
  • Kiln rollers and other furnace installations
  • Glass pot for melting radioactive waste
  • Methanol and ammonia synthesis
  • Hydrogen production
  • Reformers in the chemical and petrochemical industries
  • Components in automotive exhaust systems
  • Glow plugs for diesel engines

Send Inquiry Now