Inconel 602CA Alloy Bar

Inconel 602CA Alloy Bar

Inconel 602CA (UNS N06025 / W.Nr. 2.4633) is a Ni-Cr alloy with aluminum alloying addition, stabilized by yttrium and zirconium. It has great resistance to oxidizing atmospheres, high-temperature strength, and creep properties.
Send Inquiry

Inconel 602CA (UNS N06025 / W.Nr. 2.4633) is a Ni-Cr alloy with aluminum alloying addition, stabilized by yttrium and zirconium. It has great resistance to oxidizing atmospheres, high-temperature strength, and creep properties.

 

A relatively high carbon content combined with the alloying additions of titanium and zirconium results in high creep rupture strength. Inconel 602 CA provides 150% of the strength of other commonly used nickel alloys such as alloy 600.

 

Inconel 602CA alloy bar is the most oxidation resistant/high strength nickel alloy available. It is capable of extreme temperature use up to and beyond 2200°F (1200°C). For thermal processing applications where minimal product contamination is necessary, the oxidation/scaling resistance of alloy 602CA is extremely desirable. A high chromium content, along with aluminum and yttrium additions, allows the alloy to develop a tightly adhering oxide scale.

 

As a leading Inconel Alloy supplier in China, Lork Group manufactures and produces Inconel 602CA alloy bar of various sizes. Contact us as your Stock Distributor and Supplier.

 

Chemical Composition

 

Element

Content (MAX)

Cr

26.00

Ni

Balance

C

0.25

AI

2.40

Ti

0.20

Y

0.12

Zr

0.10

Mn

0.15

Si

0.50

Cu

0.10

Fe

11.00

 

Inconel 602CA Alloy Bar Application

 

  • Radiant tubes
  • Furnace muffles
  • Rotary and shaft furnaces
  • Kiln rollers and other furnace installations
  • Glass pot for melting radioactive waste
  • Methanol and ammonia synthesis
  • Hydrogen production
  • Reformers in the chemical and petrochemical industries
  • Components in automotive exhaust systems
  • Glow plugs for diesel engines
  • pipes in concentrating solar power (CSP) plants
  • cooling of syngas during E-Fuel production

 

 

Manufacturing Process

 

product-1200-682

 

Main Applications

 

product-1200-833

 

Packaging & Shipping

 

product-1200-690

product-1200-1147

 

FAQS

 

If you have any other questions, please contact me!

 

Q: Can you produce nickel alloy bars?

A: Yes, we can produce nickel alloy bars according to your requirements.

Q: What is your minimum order quantity?

A: Our minimum order quantity is 50 kg. Larger quantity, lower price.

Q: How long is your delivery time?

A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.

Q: Can you provide samples?

A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.

Q: How can l quickly get the price list?

A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.

Q: How do you control product quality?

A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.

Q: Can you provide processing services?

A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.

 

 

 

 