Incoloy 925
Details
Lork Group high-quality Incoloy 925 (UNS N09925) is an age-hardenable nickel-iron-chromium alloy with the addition of molybdenum, copper, titanium, and aluminium.
Products Description
Lork Group high-quality Incoloy 925 (UNS N09925) is an age-hardenable nickel-iron-chromium alloy with the addition of molybdenum, copper, titanium, and aluminium. Each of these additions plays its own part in making Alloy 925 a high-strength alloy with excellent corrosion resistance.
Incoloy 925 has excellent corrosion resistance consistent with Alloy 825. High levels of nickel ensure protection against stress corrosion cracking, whilst the additional molybdenum and copper resist reducing environments, in the same way that Chromium resists oxidising environments. Molybdenum enhances resistance to pitting and crevice corrosion, lifting the Pitting Resistance Equivalent number (PREN) to above 26.
With such a balanced composition, Alloy 925 is particularly suited to down-hole applications in sour gas wells, but can also be used in less aggressive applications as it resists general, pitting, crevice and stress corrosion cracking in most aqueous environments where chloride or sulphide ions may be present.
Product Form
Rod, Bar, Wire and Forgings: ASTM B408/ASME SB408, ASTM B564/ASME SB564, ISO 9723/9724/9725
Plate, Sheet and Strip: ASTM A240/A480/B409/B906/ASME SA240/SA480/SB409/SB906, ISO 6208
Pipe and Tube: ASTM B163/ASME SB163, ASTM B407/B829/ASME SB407/SB829, ASTM B514/B775/ASME SB514/SB775, ASTM B515/B751/ASME SB515/SB751, ISO 6207
Incoloy 925 Chemical Composition
|
Elements |
Content (%) |
|
Ni |
44 |
|
Fe |
28 |
|
Cr |
21 |
|
Mo |
3 |
|
Ti |
2.1 |
|
Cu |
1.8 |
|
Al |
0.3 |
|
C |
0.01 |
Incoloy 925 Property
|
Density, g/cm3 |
Melting Point, ℃ |
Tensile Strength, MPa |
Yield Strength, MPa |
ELongation, % |
Hardness, HB |
|
8.08 |
1311-1366 |
1210 |
810 |
24 |
– |
Incoloy 925 Application
- Power generation equipment (heat exchangers, boilers)
- Chemical processing plants
- Oil and gas production facilities
- Aerospace and marine engineering components
- Valves, pumps, and other high-performance industrial parts