Incoloy 800

Lork Group specializes in supplying Incoloy 800 bars, pipes, plates, and strips. For more product information, please click the image link below to view the details.

Incoloy 800 Nickel Alloy Bar (UNS N08800)
Incoloy 800 Alloy Pipe (ASTM B163 / ASTM B407 / ASTM B829)
Incoloy 800HT Nickel Alloy Sheet (UNS N08811)
Incoloy 800 Nickel Alloy Strip (UNS N08800)
page-600-600

Details

 

Lork Group's high-quality Incoloy 800 is a type of nickel-chromium-iron alloy that is known for its excellent resistance to corrosion, high-temperature oxidation, and creep.

Want the latest quotes and dimensions? Contact us today!
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Incoloy 800 is a type of nickel-chromium-iron alloy that is known for its excellent resistance to corrosion, high-temperature oxidation, and creep. Incoloy 800 tends to work harden during machining. can be welded by common welding techniques, using a matching filler metal.

Incoloy 800 is capable of remaining stable and maintaining its austenitic structure even after long-term exposure to high temperatures. Other characteristics of the alloy are good strength and high resistance to oxidizing, reducing, and aqueous environments. The standard forms in which this alloy is available are round, flat, forging stock, tube, plate, sheet, wire, and strip.

Incoloy 800 is a highly versatile alloy that is valued for its high resistance to corrosion and high-temperature oxidation, its good strength and creep resistance at high temperatures, and its good weldability. Its unique properties make it an ideal material for a wide range of applications, from the chemical processing industry to the aerospace industry.

 

Product Form

 

Bar: ASTM B408, AMS 5766

Forging: ASTM B564, AMS 5766

Sheet/Plate/Strip: ASTM B409, AMS 5871

Wire: ASTM B408

Pipe: ASTM B407, ASTM B514, ASTM B163

 

Incoloy 800 Chemical Composition

 

Element

Content (%)

Fe

≥39.5

Ni

30-35

Cr

19-23

Mn

≤1.5

Others

Remainder

 

Incoloy 800 Properties

 

Tensile Strength (σb/MPa)

Yield Strength (σp0.2/MPa)

Elongation (σ5/%)

520

205

30

 

Incoloy 800 Applications

 

  • Heat exchangers
  • Carburising equipment
  • Heating elements
  • Sheathing and nuclear steam generator tubing.

 