Lork Group's high-quality Hastelloy X (UNS N06002 / W. NR. 2.4665) is a nickel-chromium-iron-molybdenum superalloy with outstanding high-temperature strength, oxidation resistance, and fabricability.
We are available at any time to provide quotes and dimensional information-please feel free to contact us.
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488
Products Description
Lork Group's high-quality Hastelloy X (UNS N06002 / W. NR. 2.4665) is a nickel-chromium-iron-molybdenum superalloy with outstanding high-temperature strength, oxidation resistance, and fabricability. Alloy X's oxidation resistance is excellent up to 2200° F.
Hastelloy X nickel alloy has also been found to be exceptionally resistant to stress-corrosion cracking in petrochemical applications. Matrix stiffening provided by the molybdenum content results in high strength in a solid-solution alloy having good fabrication characteristics. Although this nickel alloy is primarily noted for heat and oxidation resistance, it also has good resistance to chloride stress-corrosion cracking, carburization, and excellent resistance to reducing or carburizing atmospheres. Two common conditions that often lead to early failure in high-temperature alloys, carburization and nitriding, Hastelloy X resists.
Product Form
Bar and forgings: ASTM B572, AMS 5754
Sheet, Strip and Plate: ASTM B435, AMS 5536
Wire: ASTM B166, AMS 5798
Pipe: ASTM B622/ASTM B619/ASTM B626/AMS 5588/AMS 5587
Hastelloy X Chemical Composition
|
Composition |
Content(%) |
|
|
Min |
Max |
|
|
Ni |
Bal. |
|
|
Cr |
20.5 |
23 |
|
Fe |
17 |
20 |
|
Mo |
8 |
10 |
|
W |
0.2 |
1 |
|
Co |
0.5 |
2.5 |
|
C |
0.05 |
0.15 |
|
Mn |
- |
1 |
|
Si |
- |
1 |
|
S |
- |
0.015 |
|
Cu |
- |
0.5 |
|
AI |
- |
0.15 |
|
Ti |
- |
0.5 |
Hastelloy X Properties
|
Tensile Strength (σb/MPa) |
Yield Strength (σp0.2/MPa) |
Elongation (σ5/%) |
|
690 |
275 |
30 |
Hastelloy X Application
- Gas turbines
- Petrochemical industry
- Industrial furnaces
- Heat treating equipment
- Nuclear engineering
- Jet engine combustion chambers
- Aircraft cabin heaters