Pure Rhenium Bar
A Rhenium Bar is a solid form of the rare transition metal rhenium (Re), known for its exceptional properties and specialized applications. Offer remarkable stability at extremely high temperatures, maintaining their structural integrity even in environments exceeding 3000°C. This makes them indispensable in applications like aerospace, nuclear reactors, and high-performance engines.
Email: susan@lorkgroup.com
WhatsApp: +86 19937075488
Key Properties of Rhenium Bar
- High Melting Point: ~3,180°C (one of the highest among metals, surpassed only by tungsten and carbon).
- Density: ~21 g/cm³ (similar to platinum, making rhenium bars extremely heavy for their size).
- Ductility: Retains malleability even at high temperatures, unlike brittle refractory metals like tungsten.
- Corrosion/Oxidation Resistance: Stable in harsh environments, especially at elevated temperatures.
- Rarity: One of Earth's least abundant elements, typically extracted as a byproduct of molybdenum and copper ore processing.
Rhenium Bar Specifications
|
Specifications |
4N Grade Re>99.99%(calculated by subtraction method, except gas element) |
|
|
5N Grade Re>99.999%(calculated by subtraction method, except gas element) |
|
Appearance |
Grey or silver metallic square bar or round bar |
|
Sizes |
Square bar (12~16) *(12~16)* (150~500) mm |
|
|
Round bar D(10~20) *L (50~300) mm. Can be customized as per requirement |
Chemical Composition
Main content: Re 99.95% min (excluding gas elements)
Maximum trace metallic impurities, analysed by ICP-MS
|
Trace Impurities (%, max) |
|||||
|
Element |
4N Grade |
5N Grade |
Element |
4N Grade |
5N Grade |
|
Na |
0.0010 |
0.0001 |
Ni |
0.0001 |
0.00001 |
|
Mg |
0.0001 |
0.00001 |
Cu |
0.0001 |
0.00001 |
|
Al |
0.0001 |
0.00001 |
Zn |
0.0001 |
0.00001 |
|
Si |
0.0005 |
0.00005 |
As |
0.0001 |
0.00001 |
|
P |
0.0001 |
0.00005 |
Zr |
0.0001 |
0.00001 |
|
K |
0.0010 |
0.0001 |
Mo |
0.0010 |
0.0002 |
|
Ca |
0.0005 |
0.00005 |
Cd |
0.0001 |
0.00001 |
|
Ti |
0.0001 |
0.00001 |
Sn |
0.0001 |
0.00001 |
|
V |
0.0001 |
0.00001 |
Sb |
0.0001 |
0.00001 |
|
Cr |
0.0001 |
0.00001 |
Ta |
0.0001 |
0.00001 |
|
Mn |
0.0001 |
0.00001 |
W |
0.0010 |
0.0002 |
|
Fe |
0.0005 |
0.00005 |
Pb |
0.0001 |
0.00001 |
|
Co |
0.0001 |
0.00001 |
Bi |
0.0001 |
0.00001 |
|
Se |
0.0001 |
0.00001 |
Tl |
0.0001 |
0.00001 |
|
Gas Element for Medium Density(%, max) |
|||||
|
O |
0.03 |
0.03 |
C |
0.005 |
0.002 |
|
N |
0.003 |
0.003 |
H |
0.002 |
0.002 |
|
Gas Element for High Density(%, max) |
|||||
|
O |
0.003 |
0.003 |
C |
0.005 |
0.002 |
|
N |
0.003 |
0.003 |
H |
0.002 |
0.002 |
Application
Vacuum Equipment Manufacturing
Rhenium bars are widely employed in the production of vacuum equipment due to their superior corrosion resistance. They are critical in the fabrication of components like vacuum tubes, furnaces, and other devices that operate in low-pressure environments, ensuring durability and reliability.
Semiconductor Manufacturing
In semiconductor production, Rhenium bars are indispensable for crafting electrodes and connectors in electronic components. Their high electrical conductivity and thermal stability make them ideal for applications that demand precision and consistent performance.
Medical Devices
Rhenium bars play a crucial role in the manufacturing of medical devices, particularly those that require biocompatibility and reliability. Their unique properties ensure that medical instruments and implants maintain their performance in demanding conditions, contributing to advancements in healthcare technology.
Aerospace
In the aerospace industry, Rhenium bars are employed in the construction of jet engine components such as turbine blades and combustion chambers. Their ability to withstand extremely high temperatures and mechanical stresses makes them essential for maintaining the efficiency and safety of modern aircraft.
X-ray Technology
Rhenium bars are utilized as anode materials in X-ray tubes, both for medical imaging and industrial radiography. Their contribution to X-ray technology enhances the precision and effectiveness of diagnostic tools, enabling clearer imaging and more accurate diagnostics.
Catalysis
Rhenium bars act as catalysts in various chemical reactions, particularly in the petrochemical industry. They facilitate processes such as hydrogenation and reforming, playing a critical role in the production of fuels and chemicals, thereby supporting the energy and manufacturing sectors.
FAQ

Common Problem
Is it prone to oxidation?
Oxidation occurs at high temperatures in air; use in a vacuum or inert atmosphere is recommended.
Is a test report provided?
Includes a report on chemical composition and purity analysis.
Do you support small-batch orders?
Research samples and custom specifications are available.
What is the delivery lead time?
Generally, if the items you require are in stock, we can ship them immediately. If they are not in stock, a 15-day production period is required.
Hot Tags: Pure Rhenium Bar, Rhenium Rod, Pure Pure Rhenium Bar, Rhenium Metal Bar, High Temperature Alloy Additive, Aerospace Propulsion Bar
You Might Also Like
Send Inquiry