UNS N09901 / Nimonic 901 Bar

UNS N09901 / Nimonic 901 Bar

Nimonic 901 bars (corresponding to UNS N09901 / European grade 2.4662 / NiFeCr12Mo6Ti3 are a classic precipitation-hardening iron-nickel-chromium-based superalloy. They are typically delivered in the annealed/solution-treated state to facilitate subsequent machining by customers.
Send Inquiry

Products Description

 

 

 

Nimonic 901 Bar

Nimonic 901 is a Fe-Ni-Cr-based precipitation-hardening wrought superalloy, also known as Incoloy 901 / UNS N09901 in the Anglo-American system, and W.Nr. 2.4662 in the German standard.

It is not positioned as a "highest temperature resistant" nickel-based alloy, but rather as a turbine disk-grade material that balances high strength, creep resistance, and good forgeability in the 600–650℃ range. Widely used in turbine discs, compressor discs, shafts, and fasteners for aero engines and gas turbines.

Common Standards Comparison

American Standard: UNS N09901, AMS 5660 / 5661, ASTM B637
British Standard: BS HR 503 / HR 55
German Standard: DIN 2.4662

Nimonic 901 Bar

 

Size Reference

 

 

Standard stock/rolling range: Diameter 6mm to 200mm.

Common specifications for aerospace high-strength fasteners/small and medium-sized discs: 20mm to 100mm is common.

Customizable square bars, flat bars, and hexagonal bars are available; specific dimensions are usually customized to order.

Generally, orders start from 50kg.

 

Surface Condition and Finishing Grade

Black Bar: Hot-rolled or hot-forged bar without peeling, with an oxide scale on the surface, typically requiring subsequent machining.

Peeled/Turned Bar: Surface defects have been removed; often used for further precision machining.

Bright/Polished Bar: Centerless grinding or polishing has resulted in a high surface finish and tighter tolerances.

 

Nimonic 901 contains high levels of alloying elements such as titanium, molybdenum, and aluminum, exhibiting high deformation resistance and a narrow hot working window. It is typically manufactured using vacuum induction melting (VIM) + vacuum arc remelting (VAR) or electroslag remelting (ESR) processes. For large-diameter bars, please contact us to confirm the delivery time.

 

If you have purchasing needs or would like to learn more about pricing or dimensions, please contact us.

 Email: layla@lorkgroup.com |  WhatsApp: +86 199 3707 5488

 

Core performance and advantages

 

 

 
 

Excellent high-temperature strength and creep resistance

It can withstand long-term mechanical stress without easily undergoing plastic deformation within an operating temperature range of approximately 600°C to 650°C, making it particularly suitable for manufacturing turbine disks for aero-engines and industrial gas turbines.

 
 
 

Good thermal fatigue stability

It possesses excellent resistance to high- and low-cycle fatigue, maintaining extremely high structural integrity under complex temperature cycles and alternating loads.

 
 
 

Balancing high strength and forgeability

Due to its higher iron content compared to pure nickel-based superalloys, its overall hot workability (such as forging processability) is more balanced, making it more suitable for the blanking and forming of large-section forgings.

 

 

chemical composition

 

 

Ni 40.0-45.0
Fe Balance
Cr 11.0-14.0
Mo 5.0-6.5
Ti 2.0-3.1(Usually 2.2-2.75)
Al ≤0.35((Usually 0.2-0.35)
C 0.01-0.08((Usually ≤0.06)
Mn ≤0.50
Si ≤0.60
S/P S≤0.015, P≤0.03
B 0.01-0.02
Co ≤1.0(Some standard operating values ​​are ≤1.5)

 

Physical properties

 

 

Density 8.14g/cm³
Melting temperature range 1280-1345°C
Elastic modulus 205-210GPa
Thermal conductivity(room temperature) 11.5-13.1W/(m·K)
Specific heat capacity 435J/(kg·K)
Resistivity  

 

Mechanical properties

 

 

Tensile strength 1200-1450MPa
0.2% Yield strength 850-1050MPa
Elongation 10-18%
Reduction of area 20-35%
Hardness HRC 35-40

 

Procurement Considerations

 

 

Nimonic 901 Bar

Material Standards and Certifications: Confirm compliance with aerospace standards such as AMS 5660, AMS 5661, or ASTM B637. Verify chemical composition and mechanical properties.

Metallurgical Process Traceability: Aerospace applications typically require a dual process of VIM + VAR (vacuum induction melting + vacuum arc remelting) to effectively control inclusions and ensure internal purity.

Delivery Status Confirmation: Clarify whether the product is in "Annealed/Solution Treated" or "Aged" condition. Most machining plants require solution-treated delivery for easier subsequent part forming.

 

Contact now

 

Lork Group
Marketing Operations Department

Hot Tags: Nimonic 901 Bar, UNS N09901, EN 2.4662, Iron-nickel-chromium based superalloys, precipitation-hardening superalloys, superalloy round bars, aerospace-grade discs

Send Inquiry