Waspaloy





Details
Lork Group high-quality Waspaloy is a high-strength, nickel-based superalloy known for its excellent high-temperature mechanical properties and corrosion resistance.
Products Description
Lork Group high-quality Waspaloy is a high-strength, nickel-based superalloy known for its excellent high-temperature mechanical properties and corrosion resistance. Widely used in demanding applications that require strength retention and performance at elevated temperatures, such as gas turbine engines, aerospace components, and high-temperature structural applications.
Waspaloy exhibits impressive mechanical properties, capable of achieving a tensile strength of 1103 MPa (160,000 psi) and a yield strength of 724 MPa (105,000 psi) in the age-hardened condition.
Heat treatment of Waspaloy typically involves solution annealing at a minimum of 1038°C (1900°F). This treatment optimizes the alloy's mechanical properties and helps eliminate any residual stresses.
Waspaloy offers excellent resistance to high-temperature oxidation and corrosion. It can withstand aggressive environments, including sulfuric acid, nitric acid, hydrochloric acid, saltwater, and oxidizing/reducing conditions. This corrosion resistance makes it suitable for applications exposed to various corrosive atmospheres.
Product Form
Rod, Bar, Wire and Forging Stock
ASTM B 637, ISO 9723, ISO 9724, ISO 9725, AMS 5704, AMS 5706, AMS 5707, AMS 5708, AMS 5709, AMS 5828, MAM 5706, AECMA PrEN 2193, AECMA PrEN 2194, AECMA PrEN 2406, AECMA PrEN 2958, AECMA PrEN 2959, AECMA PrEN 2960, AECMA PrEN 3220.
Plate, Sheet and Strip
AMS 5544, AECMA PrEN 2195
Other
UNS N07001, W. Nr 2.4654, MSRR 7192
Waspaloy Chemical Composition
|
Element |
Min |
Max |
|
Ni |
Balance |
|
|
Cr |
18 |
21 |
|
Co |
12 |
15 |
|
Mo |
3.5 |
5 |
|
Al |
1.2 |
1.6 |
|
C |
0.02 |
0.10 |
|
Mn |
- |
0.1 |
|
Si |
- |
0.15 |
|
P |
- |
0.015 |
|
S |
- |
0.015 |
Waspaloy Property
|
Tensile Strength |
145,000 psi (1000 MPa) maximum |
|
Yield Strength |
85,000 psi (552 MPa) maximum |
|
Elongation |
35% minimum (in 2-inch gauge length) |
|
Hardness |
HRB 99 maximum |
Waspaloy Application
- Combustion chamber
- Disks
- Blades
- Vanes
- Casings
- Shaft exhaust system