Lork Group high-quality UNS S32205 is a chromium-nickel-molybdenum-nitrogen stainless steel.UNS S32205 has superior resistance to chloride pitting and crevice corrosion.

 

Products Description

 

Lork Group high-quality UNS S32205 is a chromium-nickel-molybdenum-nitrogen stainless steel. It is the most popular grade of duplex stainless steel and has a yield strength that is twice as high as that of austenitic stainless steel standard grades. UNS S32205 consists of around 40-50% ferrite in the annealed condition. The duplex microstructure has the high strength of the ferritic grades whilst retaining the corrosion resistance of the austenitic grades.

UNS S32205 has superior resistance to chloride pitting and crevice corrosion as compared to 317L stainless steel. The alloy has outstanding corrosion resistance to seawater and most concentrations of sulphuric acid. In addition, UNS S32205 duplex stainless is also resistant to sulphide stress corrosion cracking (sour-gas environments).

 

Product Form

 

Sheet

Pipes

Bars

Coil

Plate

Plate coil

 

UNS S32205 Chemical Composition

 

Element

Content

Cr

21-23%

Ni

4.5-6.5%

Mn

2% Max

Mo

2.5-3.5%

N

0.08-0.20%

P

0.30% max

C

0.030% max

 

UNS S32205 Mechanical Properties

 

Grade

Tensile Str
(MPa) min

Yield Strength
0.2% Proof
(MPa) min

Elongation
(% in 50mm) min

Hardness

Rockwell C (HR C)

Brinell (HB)

2205

621

448

25

31 max

293 max

 

UNS S32205 Applications

 

This unique mix of materials makes UNS S32205 the right choice for a number of different critical applications in a range of industries, including:

  • Chemical processing, transport, and storage
  • Marine and Land cargo tanks
  • Biofuel production
  • Food processing
  • Pulp and Paper Manufacturing
  • Oil and gas exploration and processing
  • Waste management
  • High chloride environments

 