Lork Group high-quality Ti3Al2.5V Titanium alloy offers good corrosion resistance in oxidising, neutral and mildly reducing media, including chlorides.

 

Products Description

 

Lork Group high-quality Titanium Ti3Al2.5V (grade 9) or more simply known as Ti-3-2.5 is commonly grouped with the commercially pure grades due to it's ability to be cold rolled.

Ti3Al2.5V Titanium alloy offers good corrosion resistance in oxidising, neutral and mildly reducing media, including chlorides. Titanium Grade 18 with the addition of palladium offers greater resistance to corrosion. The alloy resists oxidation up to 600°F (316°C).

 

Product Form

 

AMS 4943 Hydraulic Seamless Tubing

AMS 4944 Hydraulic Seamless Tubing

AMS 4945 Hydraulic Seamless Tubing

ASTM B337 Gr9, ASTM B338 Gr9 & ASTM B381 Gr9 Seamless and Welded Pipe

AMS-T-9046 AB-5 Sheet, Strip, Plate

AMS-T-9047 3Al-2.5V Bar

MIL-T-9046J AD-5 Sheet, Strip, Plate

 

Titanium Ti3Al2.5V Grade 9 Chemical Composition

 

Weight %

Titanium Grade 9

Ti

bal

C

0.05

Fe

0.30

N

0.02

AI

2.5 / 3.5

O

0.12

V

2.0 / 3.0

H

0.015

Y

0.005

Other

0.40 total

 

Titanium Ti3Al2.5V Grade 9 Property

 

Material

Tensile Strength min

Yield Strength min

Elongation (%)

ksi

Mpa

ksi

Mpa

Titanium Alpha-Beta Alloy Ti-3Al-2.5V

90

621

75

517

15

Ti-3Al-2.5V Hydraulic Seamless Tubing (annealed)

 

Titanium Ti3Al2.5V Grade 9 Application

 

  • Tubing in aircraft and hydraulic systems
  • Corrosion resistant pipes and vessels
  • Recreational products - golf clubs shafts, tennis racquets, bicycle frames
  • Offshore Oil & Gas Equipment
  • Foil in honey-comb

 

Send Inquiry Now