Titanium Ti-0.15Pd Grade 7

 

product-800-800
product-600-600
product-800-800
product-600-600
product-600-600

 

Details

 

Lork Group high-quality Titanium Ti-0.15Pd Grade 7 is mechanically and physically equivalent to CP grade 2, but with the addition of palladium. The addition of palladium gives grade 7 enhanced crevice corrosion resistance at low temperatures and high PH and is the most corrosion resistant of all titanium alloys.

 

Products Description

 

Lork Group high-quality Titanium Ti-0.15Pd Grade 7 is mechanically and physically equivalent to CP grade 2, but with the addition of palladium. The addition of palladium gives grade 7 enhanced crevice corrosion resistance at low temperatures and high PH and is the most corrosion resistant of all titanium alloys.

 

Product Form

 

ASTM B265 Gr7 Sheet/plate

ASTM B338 Gr7 heat exchange tube*

ASTM B348 Gr7 bar

ASTM B367 Gr7 castings

ASTM B381 Gr7 forgings

ASTM F467 Gr7 nuts

ASTM F468 Gr7 bolts

 

Titanium Ti-0.15Pd Grade 7 Chemical Composition

 

Weight %

Titanium Grade 7

Ti

bal

C

0.10

Fe

0.30

N

0.03

Pd

0.12/0.25

O

0.25

H

0.015

Other

0.4 total max

 

Titanium Ti-0.15Pd Grade 7 Property

 

Material

Tensile Strength min

Yield Strength

Elongation (%)

ksi

Mpa

Min

Max

ksi

Mpa

ksi

Mpa

Titanium CP Grade7 Annealed Sheet

50

345

40

275

65

450

20

as per MIL-T-9046J, AMS-T-9046, AMS 4901

 

Titanium Ti-0.15Pd Grade 7 Application

 

  • Aerospace Industry: Titanium Grade 7 is used in the aerospace industry for components that require high strength, corrosion resistance, and good weldability. It is used in airframes, engine components, and structural parts, such as in the production of high-performance aircraft.
  • Marine Applications: Titanium Grade 7's excellent corrosion resistance in seawater makes it suitable for marine applications. It is used in seawater systems, propellers, and other marine equipment.
  • Chemical Processing: Titanium Grade 7's resistance to corrosion in various chemical environments makes it valuable in chemical processing equipment such as heat exchangers, reaction vessels, and pumps. It is particularly suitable for handling highly corrosive media.
  • Power Generation: Titanium Grade 7 is used in power generation applications, such as in the production of gas turbines, steam turbines, and heat exchangers, where high-temperature resistance and corrosion resistance are essential.
  • Industrial Applications: Titanium Grade 7 is used in various industrial applications, such as in the production of valves, pumps, and heat exchangers, where high strength, corrosion resistance, and good weldability are essential.
  • Medical Applications: Titanium Grade 7 is used in medical applications, such as in the production of surgical instruments and implants, where corrosion resistance and biocompatibility are essential.