Titanium Grade 4





Details
Lork Group high-quality Commercially Pure Titanium Grade 4 is the highest strength pure unalloyed Titanium with high oxygen and extra high strength. Grade 4 displays the highest strength of all the unalloyed CP grades.
Products Description
Lork Group high-quality Commercially Pure Titanium Grade 4 is the highest strength pure unalloyed Titanium with high oxygen and extra high strength. Grade 4 displays the highest strength of all the unalloyed CP grades. It combines excellent corrosion resistance with good formability and weldability.
Commercially Pure Titanium Grade 4 Mainly used in hydraulic and instrumentation tubing. Generally chosen for its corrosion resistance in a variety of chemical process equipment as well as marine and airframe applications. It can be used for parts requiring strength up to 400 ° F and oxidation resistance to 600 ° F.
Product Form
BS 3TA6 - Sheet, strip
BS 3TA7 - Bar
BS 2TA8 - Forging stock
AMS 4901 - Sheet, strip, plate
AMS 4921 - Bar
AMS-T-9046B - Sheet, strip, plate
AMS-T-9047A CP70 - Bar
MIL-T-9046H Type 1 Comp B - Sheet, strip, plate
MIL-T-9046J CP1 - Sheet, strip, plate
MIL-T-9074G CP70 - Bar
ASTM B265 - Gr4 Sheet, plate
ASTM B338 - Gr4 heat exchanger tube
Titanium Grade 4 Chemical Composition
|
Weight % |
Titanium Grade 4 |
|
Ti |
bal |
|
C |
0.08 |
|
Fe |
0.50 |
|
N |
0.05 |
|
O |
0.40 |
|
H |
0.015 |
Titanium Grade 4 Property
|
Material |
Yield Strength |
Yield Strength |
Elongation (%) |
||
|
ksi |
MPa |
ksi |
MPa |
||
|
Titanium CP Grade 4 Annealed Sheet |
80 |
552 |
70-95 |
483-655 |
15 |
|
as per MIL-T-9046J, AMS-T-9046, AMS 4901 |
|||||
Titanium Grade 4 Application
- Aerospace
- Chemical processing markets
- Bellows
- Aircraft structural honeycomb
- Gaskets
- Aircraft skin
- Heat exchanger parts
- Implantable battery cathodes/connectors
- Stamped or etched fabrications