Titanium 6Al-2Sn-4Zr-2Mo





Details
Lork Group high-quality Titanium alloy 6Al-2Sn-4Zr-2Mo, often referred to simply as Ti-6-2-4-2, is a titanium alloy known for its exceptional strength-to-weight ratio, corrosion resistance, and heat resistance properties.
Products Description
Lork Group high-quality Titanium alloy 6Al-2Sn-4Zr-2Mo, often referred to simply as Ti-6-2-4-2, is a titanium alloy known for its exceptional strength-to-weight ratio, corrosion resistance, and heat resistance properties.
Ti-6-2-4-2 is part of the alpha-beta titanium alloy family and is primarily used in aerospace and marine applications where high strength and durability are critical. With a composition of 6% aluminum, 2% tin, 4% zirconium, and 2% molybdenum.
Ti-6-2-4-2 achieves a balance of mechanical strength and toughness, making it suitable for components subjected to high stress and operating temperatures. Its versatility extends to medical implants, sporting goods, and industrial equipment where lightweight, corrosion-resistant materials are essential for performance and longevity.
Product Form & Standard
AMS 4919 sheet, strip, plate (duplex annealed)
AMS 4975 bars, wire, rings (solution and precipitation heat treated)
AMS 4981 bars, wire, forgings (solution and precipitation heat treated)
AMS 6905 bars, wire, forgings (duplex annealed)
AMS-T-9046 AB4 sheet, strip, plate
AMS-T-9047 6Al-2Sn-4Zr-2Mo bar
Ti-6-2-4-2 Chemical Composition
|
Weight % |
Titanium 6Al-2Sn-4Zr-2Mo |
|
Al |
5.5-6.5 |
|
Sn |
1.8-2.2 |
|
Zr |
3.6-4.4 |
|
Mo |
1.8-2.2 |
|
Fe |
0.25 |
|
C |
0.05 |
|
N |
0.04 |
|
H |
0.015 |
|
O |
0.15 |
|
Other |
0.30 |
Ti-6-2-4-2 Mechanical Properties
|
Material |
Thickness |
Tensile Strength min |
Yield Strength min |
Elongation in 4D (%) |
||
|
ksi |
Mpa |
ksi |
Mpa |
|||
|
Titanium 6Al-2Sn-4Zr-2Mo Sheet (duplex annealed) Room temp |
0.025"-0.062" |
135 |
931 |
125 |
862 |
8 |
|
Titanium 6Al-2Sn-4Zr-2Mo Sheet (duplex annealed) Room temp |
0.062"-1.0" |
135 |
931 |
125 |
862 |
10 |
|
Titanium 6Al-2Sn-4Zr-2Mo Sheet (duplex annealed) Room temp |
1.0"-3.0" |
130 |
896 |
120 |
827 |
10 |
Ti-6-2-4-2 Application
- Aerospace Industry
- Military and Defense
- Marine Industry
- Energy Sector
- Chemical Processing
- Medical Devices
- Automotive Industry
- Sports and Recreation
Ti-6Al-2Sn-4Zr-2Mo (Ti-6242) is a high-strength titanium alloy known for its excellent mechanical properties, high temperature stability, and resistance to corrosion. Its versatility makes it suitable for a range of demanding applications in aerospace, military, marine, energy, and other high-performance environments.