Stellite 6B Bushing
Products Description
Stellite 6B is a cobalt-based alloy known for its excellent wear resistance, high-temperature strength, and corrosion resistance. Stellite 6B bushings are designed for demanding applications involving friction, abrasion, and harsh operating environments. They provide reliable service life in industrial equipment and other applications requiring durable wear-resistant components.

Product Specifications
Supply Forms: Bushings, Sleeves, Rings, and Custom-Machined Components
Dimensions: Custom Sizes Available
Supply Condition: As-Machined or Finished Condition, depending on Requirements
Processing Services: CNC Machining, Turning, Grinding, and Custom Manufacturing
Finished Product Requirements: Dimensional tolerances, surface roughness, and other acceptance requirements for bushings are typically specified in the drawings or procurement technical specifications.
Performance Reference
| Hardness | 33–43 HRC | King-Single | Double | Queen |
| Tensile Strength | ≥ 896 MPa | 37*37*102 | 192PCS | 476PCS |
| Yield Strength | ≥ 483 MPa | 37*37*117 | 180PCS | 420PCS |
| Density | Approx. 8.387 g/cm³ | 37*37*148 | 144PCS | 336PCS |
| Melting Temperature Range | Approx. 1265–1354°C | 37*37*163 | 108PCS | 302PCS |
What are the advantages of different machines?
The core function of Stellite 6B bushings on machines is to reduce friction and wear, lower the risk of metal seizure, maintain good wear resistance under high temperature or harsh operating conditions, and extend the service life of critical components.
| Equipment | Potential Advantages of the Stellite 6B |
| Industrial pumps | Wear-resistant and anti-galling, suitable for some corrosive media environments. |
| Valves | Wear-resistant and corrosion-resistant, suitable for some high-temperature valves. |
| Steam turbines and high-temperature equipment | Good high-temperature hardness retention. |
| Metallurgical equipment | Can handle some high-temperature and abrasive conditions. |
| Mining and conveying equipment | Can be used in some severely worn parts, but impact and particle conditions need to be evaluated. |
Note: Stellite 6B is not suitable for all bearing or bushing locations. High-speed rotation, boundary lubrication, low friction coefficient requirements, or high-impact conditions necessitate a comprehensive evaluation of the mating shaft material, lubrication, clearance, and surface finish.
Lork Group
Marketing Operations Department
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488
Hot Tags: Stellite 6B Bushing, Cobalt Alloy Bushing, Stellite 6B Wear Resistant Bushing, Stellite 6B Machined Sleeve, Industrial Pumps
You Might Also Like
Send Inquiry