CKS-500 (2J32) Alloy Wire
Iron-cobalt-vanadium-based wrought permanent magnet alloy wire
CKS-500 alloy wire is an iron-cobalt-vanadium (Fe-Co-V) based, age-hardenable, and machinable permanent magnet alloy. Through cold-drawing, a magnetic anisotropic texture is developed; subsequent aging treatment induces the precipitation of a second phase, resulting in magnetic hardening and achieving high coercivity and remanence. CKS-500 alloy wire is primarily used for manufacturing small-cross-section permanent magnet components with complex geometries-such as rotors for miniature motors, hysteresis motors, magnets for precision sensors, and components for marine compasses-where high magnetic stability and precise dimensional accuracy are required.
CKS-500 alloy wire is supplied in a cold-drawn form, typically with diameters ranging from 0.5 mm to 6 mm. It is generally delivered in either a cold-drawn or solution-annealed state, facilitating subsequent processes such as coiling, cutting, or stamping. The final magnetic properties are activated through a subsequent aging treatment. The minimum order quantity (MOQ) is 50 kg, with a standard lead time of 3–4 weeks; please inquire regarding the availability of stock for standard specifications.
chemical component
| Element | Content (wt.%) |
| C | ≤0.12 |
| Si | ≤0.50 |
| Mn | ≤0.50 |
| P | ≤0.025 |
| S | ≤0.020 |
| Ni | ≤0.70 |
| Co | 51.00–53.00 |
| V | 11.8–12.7 |
| Fe | Balance |
The above represents the compositional ranges for the specified grades; actual composition shall be determined in accordance with the applicable standards and the material test certificate.
magnetic property
| Magnetic field strength Hc | ≥27.86 kA/m |
| Magnetic flux density Br | ≥0.85 T |
| Br·Hc | ≥24 kJ/m³ |
The data provided above serve as reference indicators for the wire material; specific testing conditions and acceptance requirements shall be governed by the applicable standards and the agreement between the supplier and the purchaser.
Typical mechanical properties
| Tensile strength | 735 MPa |
| Elongation | 3-8% |
| Hardness | HRC 35–45 |
Smelting method

CKS-500 alloy wire requires high uniformity in chemical composition and strict control over impurities. During production, a vacuum induction melting (VIM) process is typically employed, using iron, cobalt, and vanadium as the primary raw materials, which are proportioned and melted according to specified ratios. Throughout the melting process, it is essential to precisely control the content of cobalt and vanadium while minimizing the presence of impurities such as carbon, sulfur, and phosphorus. This helps reduce non-metallic inclusions and compositional segregation, ensuring the stability of the alloy's composition.
Once melted, the alloy is cast into ingots, which then undergo homogenization, forging, and hot rolling to produce the wire blanks required for subsequent drawing. During these processing stages, heating temperatures and the degree of deformation are carefully controlled to refine the material's internal microstructure and mitigate defects originating from the as-cast state. The wire then undergoes multiple passes of cold drawing to gradually reduce its diameter, with intermediate heat treatments incorporated as needed. The final result is a CKS-500 alloy wire characterized by uniform dimensions and high surface quality.
Lork Group
Marketing Operations Department
Email: claire@lorkgroup.com
WhatsApp: +86 199 3707 5488
Hot Tags: CKS-500, 2J32, Fe-Co-V alloy wire, iron-cobalt-vanadium permanent magnet alloy, CKS-500 alloy wire, 2J32 alloy wire
You Might Also Like