Kovar

 

Kovar Alloy Rods
Kovar Alloy
page-800-800
page-600-600
page-600-600

 

Details

 

Lork Group's high-quality Kovar/UNS K94610/ASTM F15/Nilo K is a nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Used for glass-to-metal seals in applications requiring high reliability or resistance to thermal shock.

 Ι claire@lorkgroup.com                 Ι +86 19937075488

 

Products Description

 

Lork Group high-quality Kovar/UNS K94610/ASTM F15/Nilo K is a nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, matches the expansion rate of borosilicate glasses and alumina ceramics.

Kovar (Alloy K) is used for glass-to-metal seals in applications requiring high reliability or resistance to thermal shock. Kovar (Alloy K) is used for high-power transmitting valves, transistor leads and headers, integrated-circuit lead frames, and photography flash bulbs.

Since Kovar Alloy is tough and versatile, while employing extensive quality controls throughout UNS K94610 alloy's manufacturing process to ensure uniform physical and mechanical properties for ease in deep drawing, stamping and machining are consistently achieved. Furthermore, the coefficient of thermal expansion (CTE) of Kovar is its most dynamic mechanical property.

 

Product Form

 

ASTM F 15

Wire: AMS 7726

Bars and Forgings: AMS 7727

Sheet, Strip and Plate: AMS 7728

 

Kovar/UNS K94610 Chemical Composition

 

Element

Content

Ni

29.0

Fe

53.0

Co

17.0

C

0.04 max

Mn

0.50 max

Si

0.20

AI

0.10 max

Cr

0.20 max

Mg

0.10 max

Zr

0.10 max

Ti

0.10 max

Cu

0.20 max

Mo

0.20 max

 

Kovar/UNS K94610 Property

 

Material

Condition

Yield Strength (0.1% Offset)

Tensile Strength

Elongation %

psi

MPa

psi

MPa

Alloy K Kovar

Annealed

49,000

340

75,000

520

42

 

Kovar/UNS K94610 Application

 

  • Hermetic seals
  • Power tubes
  • Microwave tubes
  • Diodes
  • Transistors
  • X-ray tubes

 

Send Inquiry Now