Kovar Alloy

Kovar Alloy

Lork Group stock and supply a wide range of kovar alloy products and materials. Including Kovar Bar, Rod, Tube, Sheet, Strip, Coil, Plate and Wire.
Send Inquiry

Lork Group stock and supply a wide range of kovar alloy products and materials. Including Kovar Bar, Rod, Tube, Sheet, Strip, Coil, Plate and Wire.

 

Kovar alloy (Alloy K) is a nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, matches the expansion rate of borosilicate glasses and alumina ceramics.

 

Kovar alloy (Alloy K) is used for glass-to-metal seals in applications requiring high reliability or resistance to thermal shock. used for high-power transmitting valves, transistor leads and headers, integrated-circuit lead frames, and photography flash bulbs.

 

kovar alloy sheet

Technical Specifications

 

ASTM

UNS

Workstoff

AMS

F15

K94610

1.3981

I-23011 CL1

 

Chemical Composition

Element

Weight

Ni

29

Co

17

Fe

Balance

Mn

0.5

Si

0.2

C

0.04

 

Coefficient of Thermal Expansion

30-300°C

10-6/°C

5

30-400°C

10-6/°C

5.15

Density

g/cm³

8.26

Curie Temp

°F
(°C)

815
(435)

Melting Point

°F
(°C)

2640
(1449)

Modulus of Elasticity at 20°C

MPa

207

Specific Heat

J/g- °C

0.11

Thermal Conductivity at 20°C

W/m.k

17.3

Thermal Expansion

W.m-¹°C

0.17

Electrical Resistivity

mm²/m

49

Poisson's coefficient

 

0.317

 

Mechanical Properties

Metallurgical Condition

Annealed, Descaled

 

Yield Strength

KSI (MPa)

40 (276)

Tensile Strength

KSI (MPa)

75 (518)

Hardness

HB

78

Elongation

50mm

>20

 

Applications

  • Hermetic Sealing
  • Electronic tubes (power, X-Ray)
  • Hybrid circuit casings
  • Oscillator housings
  • Concentrated solar power
  • Scientific instruments

 

Speak to us

We can distribute metals across the globe, including locations in Europe, the Middle East, the Far East, and the Americas.

Our address

Block B Shenglong City, Xinghua South Street, Erqi District, Zhengzhou City, Henan Province, China

Phone Number

speak to us
 

Hot Tags: Kovar Alloy,Kovar,UNS K94610,ASTM F15,W.Nr. 1.3981, Nilo K, Dilver P, Pernifer 2918, Controlled Expansion Alloy

Send Inquiry