Inconel 713C

We supply bar and plate products; please click the image below for more information on Inconel 713C profiles.

Inconel 713C Nickel Alloy Bar
page-600-600
Inconel 713C Nickel Alloy Plate
page-600-600
page-600-600

Details

 

Lork Group's high-quality Inconel 713C is a precipitation-hardening nickel-chromium-based cast alloy. It possesses excellent strength properties up to 1800ºF (980ºC). The alloy has good castability and excellent resistance to oxidation and thermal fatigue.

Contact us for a detailed quote or to inquire about custom sizing services.
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Inconel 713C is a precipitation-hardening nickel-chromium-base cast alloy. It possesses excellent strength properties up to 1800ºF (980ºC). The alloy has good castability and excellent resistance to oxidation and thermal fatigue.

Inconel 713C composition is simple and has a low density, making it ideal for hot isostatic pressing and subsequent heat treatment, improving plasticity and fatigue properties while restoring the structure and performance of parts.

 

Product Form

 

Cast Billet

Cast Round Bar

 

Inconel 713C Chemical Composition

 

CHEMICAL ANALYSIS

C

0.08/0.20

Mn

0.25 max

Si

0.50 max

Cr

12.0/14.0

Mo

3.80/5.20

Cb + Ta

1.80/2.80

Al

5.50/6.50

Ti

0.50/1.00

Cu

0.50 max

Fe

2.50 max

B

.005/.015

Zr

0.05/0.15

 

Inconel 713C Property

 

The AMS 5391 specification for alloy 713C requires the following mechanical properties in the as cast condition.

 

0.2% Yield Strength, psi

Tensile Strength, psi

Elong, % in 4D

HRC

100

110

3 min

30-42

 

Inconel 713C Application

 

  • Automotive industry (turbochargers)
  • Engine construction (compressors, impellers)
  • Plant engineering (aggressive media)
  • Racing (valves, manifolds)

 

 