Incoloy 825





Details
Lork Group high-quality Incoloy 825 is a nickel-iron-chromium alloy renowned for its exceptional resistance to a wide range of corrosive environments, including those containing chloride ions, sulfuric acid, and phosphoric acid.
Products Description
Lork Group high-quality Incoloy 825 is a nickel-iron-chromium alloy renowned for its exceptional resistance to a wide range of corrosive environments, including those containing chloride ions, sulfuric acid, and phosphoric acid. It's particularly resistant to pitting and crevice corrosion, making it ideal for applications in harsh conditions like seawater, acidic or alkaline solutions, and high-temperature water.
Beyond its use in chemical processing, power generation, and oil and gas production, Incoloy 825 finds applications in various industries, including aerospace, marine engineering, and the manufacture of heat exchangers, valves, and pumps.
Product Form
Sheet, Strip and Plate: BS3072 NA16/BS 3073 NA16/ASTM/B424/ ASTM B906/
ASME SB424/ASME SB906/DIN 17750/VdTUV 432
Pipe and Tube: BS 3074 NA16/ASTM B163, ASME SB163,ASTM B423, ASME SB423,ASTM B704, ASME SB704,ASTM B705, ASME SB705, ASTM B751, ASME SB751, ASTM B755, ASME SB755, ASTM B829, ASME SB829, DIN 17751, VdTUV 432
Rod, Bars, Forgings: BS 3076 NA16, ASTM B425, ASTM B564, ASME SB425
ASME SB564, ASME Code Case N-572, DIN 17752, DIN 17753, DIN 17754, VdTUV 432, ASTM B36
Incoloy 825 Chemical Composition
|
Element |
Content (%) |
|
Ni |
38-46 |
|
Fe |
22 |
|
Cr |
19.5-23.5 |
|
Mo |
2.50-3.50 |
|
Cu |
1.50-3.0 |
|
Mn |
1 |
|
Ti |
0.60-1.20 |
|
Si |
0.50 |
|
Al |
0.20 |
|
C |
0.050 |
|
S |
0.030 |
Incoloy 825 Property
|
Material |
Material |
Tensile Strength MPa |
Yield Strength (0.2% Offset) MPa |
Elongation (%) |
|
Alloy 825 Tube |
Annealed |
772 |
441 |
36 |
|
Alloy 825 Tube |
Cold Drawn |
1000 |
889 |
15 |
|
Alloy 825 Bar |
Annealed |
690 |
324 |
45 |
|
Alloy 825 Plate |
Annealed |
662 |
338 |
45 |
|
Alloy 825 Sheet |
Annealed |
758 |
421 |
39 |
Incoloy 825 Applications
- Acid production piping
- Vessels
- Pickling
- Chemical process equipment