Incoloy 800HT

We offer bars, tubes, and plates. Want to know more? Click the image below for details.

Incoloy 800HT Nickel Alloy Bar (UNS N08811)
Incoloy 800HT Nickel Alloy Pipe (UNS N08811)
Incoloy 800HT Nickel Alloy Sheet (UNS N08811)
page-600-600
page-600-600

Details

 

Lork Group's high-quality Incoloy 800HT (UNS N08811 / W.Nr. 1.4959) is a nickel-chromium-iron alloy that is known for its excellent resistance to corrosion, high-temperature oxidation, and creep.

Need a quote or size information? Feel free to contact us!
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Lork Group's high-quality Incoloy 800HT (UNS N08811 / W.Nr. 1.4959) is a high-temperature alloy that is similar to Incoloy 800H, but with a slightly different composition and properties. It is a nickel-chromium-iron alloy that is known for its excellent resistance to corrosion, high-temperature oxidation, and creep.

Incoloy 800HT has a higher carbon content than Incoloy 800H, which gives it improved strength and creep resistance at high temperatures. It also has a higher titanium content, which helps to reduce the risk of sensitization.

Incoloy 800HT is used in applications where high-temperature strength and resistance to oxidation and corrosion are critical, such as in heat exchangers, boilers, and other high-temperature equipment in the power generation and chemical processing industries. It is also used in the aerospace industry and in marine engineering. It is valued for its excellent high-temperature properties, corrosion resistance, and weldability, making it an ideal material for a wide range of industrial applications.

 

Product Form

 

Rod, Bar, Wire and Forgings: ASTM B408/ASME SB408, ASTM B564/ASME SB564, ISO 9723/9724/9725

Plate, Sheet and Strip: ASTM A240/A480/B409/B906/ASME SA240/SA480/SB409/SB906, ISO 6208

Pipe and Tube: ASTM B163/ASME SB163, ASTM B407/B829/ASME SB407/SB829, ASTM B514/B775/ASME SB514/SB775, ASTM B515/B751/ASME SB515/SB751, ISO 6207

Fitting: ASTM B366/ASME SB366

 

Incoloy 800HT Chemical Composition

 

Elements

Content (%)

Fe

≥ 39.5

Ni

30- 35

Cr

19-23

Mn

≤ 1.50

Si

≤ 1

Cu

≤ 0.75

Ti

0.15-0.60

Al

0.15-0.60

C

0.060-0.10

S

≤ 0.015

 

Incoloy 800HT Property

 

Density, g/cm3

Melting Point, ℃

Tensile Strength, MPa

Yield Strength, MPa

ELongation, %

Hardness, HB

8.00

1357-1375

531

200

52

–

 

Incoloy 800HT Application

 

  • Heat exchangers
  • Boilers
  • High-temperature equipment in the power generation industry
  • High-temperature equipment in the chemical processing industry
  • Aerospace industry
  • Marine engineering
  • Valves
  • Pumps
  • Other high-temperature components

 

 

Send Inquiry Now