Incoloy 800

Our Lork Group supplies bars, tubes, plates, and strips. For more details, please click the image below to jump to the link.

Incoloy 800 Nickel Alloy Bar (UNS N08800)
Incoloy 800 Alloy Pipe (ASTM B163 / ASTM B407 / ASTM B829)
Incoloy 800 Nickel Alloy Sheet (UNS N08800)
Incoloy 800 Nickel Alloy Strip (UNS N08800)
page-600-600

Details

 

Incoloy 800 (Unified designation UNS N08800) is a nickel-iron-chromium-based austenitic alloy that reduces the nickel content to save costs while maintaining good heat and corrosion resistance.

Want the latest quotes and sizes? Contact us now!

📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Incoloy 800 (UNS N08800 / W.Nr. 1.4876) is a nickel-iron-chromium alloy renowned for its excellent resistance to high-temperature oxidation, carburization, and corrosion. Its good metallurgical stability and machinability make it suitable for harsh industrial environments. It is widely used in petrochemical processing equipment, heat exchangers, industrial furnaces, heat treatment equipment, and electric heating systems.

 

Corresponding standard

 

  • Seamless pipes and fittings ASTM B407
  • Heat exchanger tubes ASTM B163
  • Bars and strips ASTM B408
  • Bars, forgings and forging billets AMS 5766
  • Plates, sheets and strips ASTM B409 AMS 5871
  • Welded pipes ASTM B514 ASTM B515
  • Forgings ASTM B564
  • Fittings ASTM B366

 

Incoloy 800 Chemical Composition

 

Element

Minimum %

Maximum %

Ni

30.00

35.00

Cr

19.00

23.00

Fe

39.50

Balance

C

--

0.10

Mn

--

1.50

Si

--

1.00

Al

0.15

0.60

Ti

0.15

0.60

Cu

--

0.75

S

--

0.015

P

--

0.030

Note: The upper limit for phosphorus content may vary depending on the product standard, and some product specifications may use different limits. Please refer to the version of the standard being implemented for specific details.

 

Incoloy 800 Physical properties

 

Density

7.94 g/cm³

Melting Range

1357–1385°C

Specific Heat Capacity (0–100°C)

460 J/(kg·K)

Thermal Conductivity (approx. 20°C)

11.5 W/(m·K)

Electrical Resistivity (approx. 20°C)

0.989 μΩ·m

Modulus of Elasticity (approx. 20°C)

196.5 GPa

 

Incoloy 800 Mechanical properties

 

Tensile Strength

≥520 MPa

Yield Strength (0.2% Offset)

≥205 MPa

Elongation

≥30%

Hardness

Approx. 138 HB, typical value HB

 

Incoloy 800 Application

 

  • Petrochemical Industry: Cracking furnace components, process piping, high-temperature treatment equipment
  • Heat Treatment Equipment: Furnace tooling, heat treatment trays, support components
  • Heat Exchangers: Heat exchange tubes, heat exchanger components
  • Industrial Furnaces: Furnace internal structural components, heating equipment components
  • Electric Heating Equipment: Heating element sheaths, heating system components
  • Chemical Processing: Chemical equipment components, corrosion-resistant structural components.