Haynes282 alloy (UNS N07208) is a nickel-based superalloy, known for its exceptional high-temperature strength, excellent creep and fatigue resistance, and superior oxidation and corrosion resistance.

We are ready to provide quotes and size consultations; please feel free to contact us.
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Products Description

 

Haynes282 alloy (UNS N07208) is a nickel-based superalloy, known for its exceptional high-temperature strength, excellent creep and fatigue resistance, and superior oxidation and corrosion resistance. The exceptional combination of mechanical properties, thermal stability, and corrosion resistance of Haynes 282 makes it a valuable material for applications where reliable performance under extreme conditions is essential. Its versatility and suitability for high-temperature environments have contributed to its widespread adoption in various industries.

Haynes 282 exhibits exceptionally high tensile and yield strengths, even at temperatures up to 1800°F (982°C). It maintains its strength and ductility at these elevated temperatures, making it well-suited for use in demanding high-temperature applications. The alloy also demonstrates excellent creep resistance, allowing it to withstand long-term exposure to high stresses and temperatures without significant deformation.

 

One of the key features of Haynes 282 is its superior oxidation and corrosion resistance. The formation of a protective oxide layer on the alloy's surface helps it withstand harsh, high-temperature environments, such as those encountered in gas turbine engines, industrial furnaces, and chemical processing equipment. This resistance to oxidation and corrosion makes Haynes 282 a preferred choice for applications where exposure to aggressive environments is a concern.

 

Haynes 282 finds widespread use in the aerospace, power generation, and chemical processing industries. In the aerospace sector, it is commonly employed in components like turbine blades, vanes, and combustion chambers, where its high-temperature strength, fatigue resistance, and oxidation resistance are critical. In power generation, the alloy is used in steam turbine parts and boiler equipment. It also sees application in the petrochemical industry, particularly in reactors, heat exchangers, and other process equipment operating at elevated temperatures.

 

Product Form

 

Plate/Sheet/Strip

Forgings/Bar

 

Haynes 282 Chemical Composition

 

Element

Min %

Max %

Al

1.38

1.65

B

0.003

0.01

C

0.04

0.08

Nb

–

0.20

Co

9.00

11.00

Cr

18.50

20.50

Cu

–

0.10

Fe

–

1.50

Mn

–

0.30

Mo

8.00

9.00

Ni

bal

 

P

–

0.015

S

–

0.015

Si

–

0.15

Ta

–

0.10

Ti

1.90

2.30

W

–

0.50

 

Haynes 282 Property

 

Solution-annealed and Age-hardened Sheet*

Temperature

Yield Strength 0.2% Offset

Ultimate Tensile Strength

Elongation

°F

°C

ksi

MPa

ksi

MPa

%

RT

RT

101.4

699

164.2

1132

30

1000

538

91.6

632

139.3

960

36

1200

649

91.5

631

145.7

1005

27

1300

704

90.5

624

136.5

941

24

1400

760

88.7

612

120.8

833

22

1500

816

82.3

567

100.3

692

24

1600

871

72.6

501

80.5

555

31

1700

927

43.9

303

50.2

346

37

1800

982

18.7

129

24.5

169

61

 

Solution-annealed and Age-hardened Plate

Temperature

Yield Strength 0.2% Offset

Ultimate Tensile Strength

Elongation

Reduction of Area

°C

ksi

MPa

ksi

MPa

%

%

RT

103.7

715

166.4

1147

30

31

538

94.1

649

143.8

991

34

36

649

93.2

643

152.0

1048

31

31

704

94.2

649

141.8

978

29

28

760

91.1

628

124.2

856

22

24

816

83.4

575

102.8

709

28

31

871

73.6

507

82.1

566

31

42

927

44.9

310

52.1

359

50

69

982

19.1

132

25.3

174

71

91

 

Haynes 282 Application

 

  • Sheet fabrications
  • Rings
  • Cases found in compressor
  • Combustion and turbine sections
  • Engines for aircraft
  • The transition sections and other hot-gas-path components in land-based gas turbines.

 

Send Inquiry Now