Hastelloy W





Details
Lork Group high-quality Hastelloy W (UNS N10004) is a solid-solution-strengthened super alloy that was developed primarily as a filler metal for welding of dissimilar alloys. It displays excellent dissimilar welding characteristics, and is widely used for that purpose in the gas turbine and aerospace industries.
Products Description
Lork Group high-quality Hastelloy W (UNS N10004) is a solid-solution-strengthened super alloy that was developed primarily as a filler metal for welding of dissimilar alloys. It displays excellent dissimilar welding characteristics, and is widely used for that purpose in the gas turbine and aerospace industries.
The properties of dissimilar weld joints made with alloy W are dependents upon the alloys joined, but are generally acceptable for a wide variety of combinations. Alloy W is also used as a wrought alloy for a limited number of ring-type Applications in older gas turbine engines. Haynes 242 alloy is a more modern alloy, and should be considered as a substitute for alloy W in these ring Applications.
Product Form
Rod, Bar, Wire and Forgings: AMS 5786, AMS 5755
Plate, Sheet and Strip: --
Pipe and Tube: --
Welding Product: AWS A5.14 ERNiMo-3
Chemical Composition
|
Elements |
Content (%) |
|
Nickel, Ni |
63 |
|
Molybdenum, Mo |
24 |
|
Iron, Fe |
6 |
|
Chromium, Cr |
5 |
|
Cobalt, Co |
2.50 |
|
Vanadium, V |
0.60 |
Fabrication and Heat Treatment
Welding
Can be welded using all the conventional techniques.
Heat Treatment
Does not respond to heat treatment.
Annealing
Annealed at 1185°C (2165°F) for 15 min followed by quenching in water.
Applications
- Gas Turbines: Hastelloy W is utilized in gas turbine components, including combustion chambers, exhaust systems, and other high-temperature parts due to its exceptional resistance to oxidation and high-temperature stability.
- Industrial Furnaces: The alloy is employed in the construction of industrial furnaces and high-temperature processing equipment due to its ability to withstand elevated temperatures and corrosive atmospheres.
- Chemical Processing: Hastelloy W finds use in chemical processing applications where exposure to aggressive chemicals and high-temperature conditions is a concern, such as in reactors, heat exchangers, and piping systems.
- Aerospace Industry: The alloy is used in aerospace applications, particularly in components exposed to high-temperature and corrosive environments, where its exceptional strength and resistance to oxidation are crucial for reliable performance.
- Petrochemical Industry: Hastelloy W is applied in the petrochemical industry for applications involving high-temperature and corrosive environments, including components in refining processes and chemical production.