Hastelloy C22





Details
Lork Group high-quality Hastelloy C22 (UNS N06022) with enhanced resistance to pitting, crevice corrosion and stress corrosion cracking. particularly in oxidizing and reducing conditions. This alloy offers high levels of resistance to both uniform and localized corrosion.
Products Description
Lork Group high-quality Hastelloy C22 (UNS N06022) is a versatile nickel-chromium-molybdenum-tungsten alloy known for its exceptional resistance to a wide range of corrosive environments, particularly in oxidizing and reducing conditions. This alloy offers high levels of resistance to both uniform and localized corrosion, making it suitable for use in aggressive chemical processing environments and applications involving exposure to harsh chemicals.
Hastelloy C22 with enhanced resistance to pitting, crevice corrosion and stress corrosion cracking. Alloy C22 material has the high chromium content provides good resistance to oxidizing media while the molybdenum and tungsten content give good resistance to reducing media. Hastelloy C22 UNS N06022 also has excellent resistance to oxidizing aqueous media including wet chlorine and mixtures containing nitric acid or oxidizing acids with chlorine ions.
Product Form
Bar: ASTM B462 / ASTM B564
Sheet/Strip: ASTM B575/ ASTM B906
Pipe:ASTM B622/ASTM B619/ ASTM B626
Hastelloy C22 Chemical Composition
|
Composition |
Content(%) |
|
|
Min |
Max |
|
|
Ni |
Bal. |
|
|
Cr |
20 |
22.5 |
|
Fe |
2 |
6 |
|
Mo |
- |
- |
|
W |
2.5 |
3.5 |
|
Co |
- |
2.5 |
|
C |
- |
0.015 |
|
Mn |
- |
0.5 |
|
Si |
- |
0.08 |
|
S |
- |
0.02 |
|
V |
- |
0.35 |
|
P |
- |
0.02 |
|
Ti |
- |
- |
Hastelloy C22 Property
|
Tensile Strength (σb/MPa) |
Yield Strength (σp0.2/MPa) |
Elongation (σ5/%) |
|
758 |
363 |
62 |
Hastelloy C22 Application
The exceptional corrosion resistance of C22 has promoted its use in many different markets wherever harsh environments are encountered, including the chemical process, pharmaceutical, food processing, oil & gas, power generation, and the paper industries. CRA offers specialty alloy C22 seamless pipe & tube for use in multiple industries and applications, including:
- Chemical Processing
- Food Processing
- Pharmaceutical Industry
- Oil & Gas
- Power Generation
- Pulp & Paper Industries