Hastelloy B2
Lork Group specializes in supplying bars, tubes, plates, and strips. For more product details, please click the image below to visit the link.
Details
Lork Group's high-quality Hastelloy B2 is a nickel-molybdenum alloy. It offers outstanding resistance to hydrochloric acid at all concentrations and temperatures, making it well suited for chemical processing and pollution control.
We are available at any time to provide quotes and dimensional information-please feel free to contact us.
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488
Products Description
Lork Group's high-quality Hastelloy B2 is a nickel-molybdenum alloy known for its exceptional resistance to a wide range of corrosive environments. It offers outstanding resistance to hydrochloric acid at all concentrations and temperatures, making it well suited for chemical processing, pollution control, and industrial settings where exposure to this corrosive agent is common.
Additionally, Hastelloy B2 resists reducing environments such as sulfuric, acetic, and phosphoric acids, as well as stress corrosion cracking and pitting. This alloy is characterized by its high molybdenum content, which contributes to its superior corrosion resistance properties. Hastelloy B2 is also known for its excellent weldability and formability, making it a versatile material for a wide range of applications.
Hastelloy B2 is commonly used in industries such as chemical processing, oil and gas, pharmaceuticals, and pollution control due to its ability to withstand aggressive chemical environments. Overall, Hastelloy B2 is a highly reliable and versatile material that offers exceptional resistance to corrosion, making it an ideal choice for demanding industrial applications where exposure to corrosive substances is a concern.
Product Form
Pipe Smls: ASTM B622
Pipe Welded: ASTM B619
Tube Welded: ASTM B626
Sheet / Plate: ASTM B333
Bar: ASTM B335
Forging: ASTM B564
Fitting: ASTM B366
Hastelloy B2 Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
69 |
|
Molybdenum, Mo |
28 |
|
Iron, Fe |
2 |
|
Chromium, Cr |
1 |
|
Cobalt, Co |
1 |
|
Manganese, Mn |
1 |
|
Silicon, Si |
0.10 |
|
Carbon, C |
0.01 |
Hastelloy B2 Property
|
Properties |
Metric |
Imperial |
|
Tensile strength |
914 MPa |
133000 psi |
|
Yield strength (@strain 0.200%) |
396 MPa |
57400 psi |
|
Elastic modulus |
217 GPa |
31500 ksi |
|
Elongation at break (in 50.8 mm) |
55% |
55% |
|
Hardness, Brinell (converted from Rockwell B hardness) |
168 |
168 |
|
Hardness, Knoop (converted from Rockwell B hardness) |
186 |
186 |
|
Hardness, Rockwell B |
98 |
98 |
|
Hardness, Vickers (converted from Rockwell B hardness) |
241 |
241 |
Hastelloy B2 Application
- Chemical processes
- Vacuum furnaces
- Mechanical components in reducing environments