Ferralium 255

 

page-800-800
page-800-800
page-800-800
page-800-800
page-600-600

 

Details

 

Lork Group high-quality Ferralium 255 is a duplex alloy with a high strength to weight ratio with superior abrasion and cavitation resistance.

 

Products Description

 

Lork Group high-quality Ferralium 255 is a duplex alloy with a high strength to weight ratio with superior abrasion and cavitation resistance. Resistance to chloride SCC, as well as crevice corrosion and pitting. Good ductility with a high fatigue strength in marine applications. Twice the yield strength of Alloy 20, and stronger than Duplex 2205. An excellent 40°C critical pitting temperature (ASTM G48-Method A), twice that of Alloy 2205.

 

Ferralium 255 Chemical Composition

 

Element

Content

Ni

4.5-6.5

Cr

24.0-27.0

Mo

2.9-3.9

Mn

1.50Max

C

0.04Max

Si

1.00Max

Fe

Balance

 

Ferralium 255 Mechanical Property

 

0.2% Proof Stress

550 N/mm2

80 ksi

Tensile Strength

760 N/mm2

110 ksi

Elongation, 5.65√S0 and 4D

15%

 

Reduction of Area

   

Hardness (Rockwell C)

28 HRC max.

 

 

Ferralium 255 Applications

 

  • Valves
  • Pumps
  • Shafts
  • Marine environments
  • Metallurgical
  • Municipal sanitation
  • Plastics
  • Oil and gas
  • Petrochemical
  • Paper making

 

Send Inquiry Now