Lork Group high-quality CD4MCuN (UNS J93372) is casting duplex stainless steel (austenitic/ferritic) in ASTM A995and ASTM A890.

 

Products Description

 

Lork Group high-quality CD4MCuN (UNS J93372) is casting duplex stainless steel (austenitic/ferritic) in ASTM A995and ASTM A890. CD4MCuN duplex stainless steel alloys offer a combination ofenhancedmechanical properties and corrosion resistance.

 

CD4MCuN (UNS J93372) Chemical Composition

 

Element

Content

Ca

0.04% Max

Ma

1.00% Max

Si

1.00% Max

P

0.04% Max

S

0.04% Max

C

24.50 - 26.50%

Ni

4.70 - 6.00%

Mo

1.70 - 2.30%

N

0.10 - 0.25%

Co

2.70 - 3.30%

 

CD4MCuN (UNS J93372) Physical Properties

 

Yield Strength:

70 ksi Min

Tensile Strength:

100 ksi Min

Elongation at 2 in:

16% Min

 

CD4MCuN (UNS J93372) Applications

 

  • Pump and valve
  • Chemical processing
  • Petroleum refining
  • Power generation
  • Marine

 