AL-6XN

 

page-800-800
page-800-800
page-800-800
page-800-800
page-600-600

 

Details

 

Lork Group high-quality AL-6XN (UNS N08367) is a super-austenitic stainless alloy. AL-6XN has also been successfully used in a broad range of very corrosive environments including the rapidly developing biopharm markets.

 

Products Description

 

Lork Group high-quality AL-6XN (UNS N08367) is a 6% molybdenum (6 Moly), low carbon, nitrogen-bearing super-austenitic stainless alloy. The alloy was originally designed for seawater applications. AL-6XN has also been successfully used in a broad range of very corrosive environments including the rapidly developing biopharm markets.

The high strength and corrosion resistance of the AL-6XN alloy make it a better choice than the conventional duplex stainless steels and a cost effective alternative to more expensive nickel-base alloys where excellent formability, weldability, strength and corrosion resistance are essential.

 

Product Form & Standard

 

Sheet/Plate/Strip

Bar/Rod/Forgings

Tube/Pipe

Fittings

 

AL-6XN/UNS N08367 Chemical Composition

 

Element

Content (%)

C

0.03 max

Mn

2.0 max

Si

1.0 max

Cr

20.0- 22.0

Ni

23.5- 25.5

Mo

6.0- 7.0

P

0.04 max

S

0.03 max

Cu

0.75 max

N

0.18- 0.25

 

AL-6XN/UNS N08367 Mechanical Properties

 

Tensile Strength

Yield Strength

Elongation

Hardness

770 MPa

393 MPa

44%

88 HRB

 

AL-6XN/UNS N08367 Application

 

  • FGD scrubbers
  • Reverse osmosis desalination
  • Distillation columns
  • Heat exchangers
  • Biopharm tanks and fermenters
  • Pressure vessels
  • Manways
  • Agitators and mixers
  • Seawater coolers in nuclear plants

 