Lork Group high-quality AISI 321 (1.4541/X6CrNiTi18-10) is a titanium stabilized austenitic stainless steel with good general corrosion resistance.

 

Products Description

 

Lork Group high-quality AISI 321 (1.4541/X6CrNiTi18-10) is a titanium stabilized austenitic stainless steel with good general corrosion resistance. It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C).

AISI 321 resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L. It also possesses good low temperature toughness.

Stainless steel AISI 321 / 1.4541 is resistant to intercrystalline corrosion, but not to contact with seawater. The material is non-magnetic (amagnetic μr < 1.3) and can be used up to a temperature of 550 °C. In the solution-annealed state (+AT at room temperature), the material has a tensile strength of 500 to 700 N/mm², a hardness of ≤ 215 and a density of 7.9 kg/dm³.

Stainless steel AISI 321 / 1.4541 is extremely easy to weld but only moderately easy to forge. It can be used for cold forming and cold heading. This material is used, for example, in the automotive industry, in mechanical engineering or in the chemical industry.

 

Product Form & Standard

 

AMS 5510 Sheet / strip / plate
AMS 5557 Welded/seamless tube
AMS 5559 Welded / thin wall tube
AMS 5570 Seamless tube
AMS 5576 Welded tube
AMS 5645 Bars / wire / forging

 

AISI 321 Chemical composition

 

Element

Content (%)

C

≤ 0,08

Si

≤ 1,00

Mn

≤ 2,00

P

≤ 0,045

S

≤ 0,03

N

-

Cr

17,0 - 19,0

Cu

-

Mo

-

Ni

9,0 - 12,0

Ti

≤ 0,70

Mass fraction in % according to DIN EN 10088-3

 

AISI 321 Mechanical Properties

 

Material

Condition

Tensile Strength (ksi)

Yield Strength (ksi)

% Elongation

Hardness HB

Alloy 321 AMS 5510

AMS 5510 Sheet (Sol Trtd)

70-100

25

40

-

Alloy 321 AMS 5645

AMS 5645 Bar (Sol Trtd)

-

-

-

255 max

 

AISI 321 Application

 

  • Aerospace – piston engine manifolds
  • Chemical Processing
  • Expansion Joints
  • Food Processing – equipment and storage
  • Petroleum Refining – polythionic acid service
  • Waste Treatment – thermal oxidizers

 