AISI 310

 

page-800-800
page-800-800
page-800-800
page-800-800
page-600-600

 

Details

 

Lork Group high-quality AISI 310 is an austenitic stainless steel resists oxidation up to 2010oF (1100℃) under mildly cyclic conditions.

 

Products Description

 

Lork Group high-quality AISI 310 (1.4841/X15CrNiSi25-21/UNS S31000) is an austenitic stainless steel developed for use in high temperature corrosion resistant applications. AISI 310 resists oxidation up to 2010oF (1100℃) under mildly cyclic conditions.

Because of its high chromium and moderate nickel content, 310 is resistant to sulfidation and can also be used in moderately carburizing atmospheres.

The more severe carburizing atmospheres of thermal press equipment usually require nickel alloys such as 330 (UNS N08330). 310 can be utilized in slightly oxidizing, nitriding, cementing and thermal cycling applications, albeit, the maximum service temperature must be reduced. Alloy 310 also finds usage in cryogenic applications with low magnetic permeability and toughness down to -450oF (-268℃). When heated between 1202 – 1742oF (650 – 950℃) the alloy is subject to sigma phase precipitation. A solution annealing treatment at 2012 – 2102oF (1100 – 1150℃) will restore a degree of toughness.

 

Product Form

 

Sheet / strip 125ksi AMS 5501
Sheet /strip (ann) AMS 5501
Sheet / strip (ann) AMS 5513
Seamless tube AMS 5560
1/4Hd Seamless/welded AMS 5560
1/8Hd Seamless/welded AMS 5564
Welded tube AMS 5565
Seamless/welded tube AMS 5566, AMS 5567, AMS 5569
Welded tube AMS 5575

 

AISI 310 Chemical composition

 

Weight%

AISI 310

C

0.08 max

Si

1.00 max

Mn

2.0 max

P + S max

0.040 P 0.030 S

Cr

24-26

Ni

19-22

Fe

Bal

Mo

0.75 max

Cu

0.75 max

 

AISI 310 Mechanical Properties

 

AISI 310

Ultimate Tensile Strength (ksi)

Yield Strength (ksi)

Elongation %

Reduction of Area (%)

Hardness HRB

Type 310 Sheet (Sol Trtd) AMS 5521

75-100

30

40

-

95 max

Type 310 Bar (Sol Trtd) AMS 5651

-

-

-

-

187 max

 

AISI 310 Application

 

  • Cryogenic Components
  • Food Pr℃essing
  • Furnaces – burners, doors, fans, piping and recuperators
  • Fluidized Bed Furnaces – coal combustors, grids, piping, wind boxes
  • Ore Pr℃essing/Steel Plants – smelter and steel melting equipment, continuous casting equipment
  • Petrolem Refining – catalytic recovery systems, flares, recuperators, tube hangers
  • Power Generation – coal gasifier internals, pulverized coal burners, tube hangers
  • Sintering/Cement Plants – burners, burner shields, feeding and discharging systems, wind boxes
  • Thermal Pr℃essing – annealing covers and boxes, burner grids, doors, fans, muffles and retorts, recuperators, walking beams

 

Send Inquiry Now