15-5PH

 

page-800-800
page-800-800
page-800-800
page-800-800
page-600-600

 

Details

 

Lork Group high-quality 15-5 PH stainless steel is a martensitic precipitation-hardening stainless steel with approximately 15% Chromium and 5% Nickel. It has high strength, high hardness, and excellent corrosion resistance.

 

Products Description

 

Lork Group high-quality 15-5 PH, also known as also known as UNS S15500 or XM-12,is a martensitic, precipitation hardening stainless steel. Popular due to its high strength and good corrosion resistance.

15-5 PH stainless steel is a martensitic precipitation-hardening stainless steel with approximately 15% Chromium and 5% Nickel. It has high strength, high hardness, and excellent corrosion resistance. Strength can be further increased by a single low temperature heat treatment. Compared to 17-4 PH, it offers better transverse toughness and ductility; better mechanical properties in larger cross-sections, and better forgeability. It is readily weldable. It can be machined in any of the several Thermal Conditions available to this grade.

 

Product Form & Standard

 

15-5 ESR to the following specifications

AMS 5659 TYPE 2

ASTM-A-484

UNS-S15500

 

15-5 PH VAC MELT to the following specifications

AMS 5659 TYPE 1

ASTM-A-484

 

15-5 VIM COND H-1025 to the following specifications

AMS-5659 T-1 (COND H-1025)

AMS-H-6875

ASTM-A-484

ASTM-A-564 TYPE XM-12 (COND H-1025)

 

15-5 VIM COND H-1050 to the following specifications

AMS-5659 T-1 (EXC. COND)

AMS-H-6875

ASTM-A-484

ASTM-A-564 TYPE XM-12 (EXC. COND)

BAC-5619 (150-170 MIN. TENS.)

AMS 5862: Sheet, Strip and Plate.

AMS 5826: Welding Wire

 

15-5 PH Chemical Composition

 

Element

Content (%)

Fe

75

Cr

14.48

Ni

4.5

Cu

3.5

Mn

≤1

Si

≤1

Nb + Ta

0.3

C

≤0.07

P

≤0.04

S

≤0.03

 

15-5 PH Mechanical Properties

 

Properties

Metric

Imperial

Tensile Strength

1380 MPa

200000 psi

Yield Strength

1275 MPa

184900 psi

Modulus of Elasticity

200 GPa

29000 ksi

Elongation at Break

10%

10%

Hardness, Brinell

420

420

Hardness, Knoop

451

451

Hardness, Rockwell B

104

104

Hardness, Rockewell C

44.2

44.2

Hardness, Vickers

445

445

Charpy Impact

10 J

7.38 ft.lb

 

15-5 PH Application

 

  • Aerospace structural components
  • Valves
  • Gears and Shafts
  • Oil and Gas components
  • Nuclear reactor components

 

Send Inquiry Now